Abubuwan da ke shafar rushewar samfuran roba da matakan kariya

Kullum magana, roba gyare-gyaren kayayyakin dole ne a gyare-gyare ta hanyar m mold ga gyare-gyaren aiki, roba samfurin bayan high zafin jiki, high matsa lamba vulcanization, daga mold rami ko mold core ne fiye da aka sani da mold saki. Rashin rushewar ƙasa yana ɗaya daga cikin mahimman dalilan da ke haifar da lahani na samfuran roba da tasiri akan ingancin samarwa. Yana iya haifar da lahani kamar murdiya da yayyaga sassa, wasu ma suna lalata gyambon, suna kawo matsala ga samarwa na yau da kullun. Yin nazarin abubuwan da ba su da kyau waɗanda ke shafar rushewar samfuran roba yana da mahimmanci don tabbatar da ingancin samfuran, hana lahani, hana ɓarna, da haɓaka ingantaccen samarwa.


1. Abubuwan da suka shafi rushewar kayayyakin roba

Rashin rushewar samfuran roba yana nufin cewa lokacin da aka fitar da samfurin, ba zai iya faɗuwa cikin sauƙi ba. Wannan yana faruwa ne ta hanyar abubuwa masu tasiri da yawa, waɗannan abubuwan suna da rikitarwa dangane da juna, kuma girman tasiri da magana sun bambanta, musamman ciki har da ƙirar samfurin roba, ƙirar ƙirar ƙira da masana'anta, tsarin samarwa, hanyar aiki, kulawar mold, da dai sauransu.


1.1 Tasirin ƙirar samfurin roba akan sakin mold

Tsarin samfuran roba kai tsaye yana shafar aikin sakin samfuran, don haka ƙirar samfuran yakamata ya dace da buƙatun sauƙin rushewar samfuran. Babban abin da ke shafar rushewar ƙirar samfuri shine gangaren ruguzawa, don buɗe ƙirar da fitar da samfurin, saman ciki da na waje na farfajiyar rabuwar tsaye ya kamata a samar da isassun gangara. Ko da yake wasu samfuran suna da gangaren rushewa, ƙimar ta yi ƙanƙanta, wasu samfuran kuma suna da gangaren saman waje ne kawai, suna watsi da gangaren saman ciki da haƙarƙarin ciki da juriya; Wasu samfuran ba su da gangara kwata-kwata, wanda ke kawo matsala ga rushewar samfurin. Bayan an gasa samfurin, raguwar centripetal yana faruwa saboda sanyin samfurin, wanda ke haifar da babban ƙarfin riƙewa a kan ainihin ko fil, wanda ke hana rushewa. Idan an ƙaru gangaren rushewa, wannan juriya na iya raguwa sosai, kuma ana iya guje wa lahani kamar yaga samfurin saboda rashin gangara. Rushewar gangaren yana da alaƙa da siffa da kauri na samfurin, yawanci ana ƙaddara ta zahiri, kuma gangaren samfurin gabaɗaya yana tsakanin 1 ° ~ 3 °.


1.2 Tasirin ƙirar ƙira da masana'anta akan sakin mold

1.2.1 Tasirin ƙirar ƙira akan sakin ƙura

Rubber mold ne daya daga cikin manyan kayan aiki don samar da roba kayayyakin, mold matsi manufa za a iya raba allura mold, mutu simintin gyaran kafa mold, latsa mold zane ne bisa ga siffar, halaye da kuma amfani da bukatun na samfurin, bisa ga wannan roba kayayyakin tsara da dama kyawon tsayuwa na daban-daban Tsarin. Tsarin mold yana da alaƙa kai tsaye da ingancin samfuran, haɓakar samarwa, wahalar sarrafa mold da rayuwar sabis. Saboda haka, binciken ƙirar ƙirar ƙirar ƙira yana da mahimmanci. Don tabbatar da cewa samfuran roba suna da daidaitattun lissafi da takamaiman daidaiton girma, ƙirar ƙirar ƙirar yakamata ta bi ƙa'idodi masu zuwa:

(1) Jagora da fahimtar taurin, raguwa da amfani da buƙatun kayan da ake amfani da su a cikin samfuran roba.

(2) Tabbatar da siffa da kwandon samfurin.

(3) Tsarin ƙirar ya kamata ya zama mai sauƙi da ma'ana, matsayi ya kamata ya zama abin dogara, shigarwa da rarrabuwa ya kamata ya dace, kuma ya zama mai sauƙi don aiki.

(4) Yawan cavities mold ya dace, wanda ya dace don yin amfani da machining da mold, kuma ya kamata a yi la'akari da yadda ya dace.

(5) Tsarin ya kamata ya kasance yana da isasshen ƙarfi da tsayin daka, kuma yayi ƙoƙari ya zama ƙananan siffa, haske a nauyi, mai sauƙin sarrafawa, kuma daidai da tsarin samarwa.

(6) Ramin ƙura ya kamata ya dace don lodawa da fitar da samfurin, kuma lokacin vulcanizing, kayan roba yakamata su sami isasshen matsi.

(7) Tsarin ya kamata ya kasance yana da takamaiman daidaito, ƙarewa da shimfidar wuri mai ma'ana, wanda ke da sauƙin datsa.

(8) Model ya kamata ya sami karyewar tsagi na roba don sauƙaƙe tsaftacewa.

(9) The mold zane kamata dace da serialization da standardization, kuma ku yi jihãdi ga mai kyau versatility.

Daga abubuwan da ake buƙata na ƙirar ƙirar ƙira, ana iya ganin cewa abubuwan da ke shafar lalata samfuran sun haɗa da ƙin ƙurar ƙura, juriya mai lalata, tsarin fitarwa, da sauransu.

1.2.1.1 Mold taurin

Kwayoyin roba gabaɗaya suna amfani da gyare-gyaren da aka haɗa, don haka akwai tsangwama ko tazarar da ta dace a cikin gyare-gyare. A cikin tsarin samarwa, a ƙarƙashin aikin ƙwanƙwasa ƙarfi ko matsa lamba na allura, sassa na gyare-gyare suna da sauƙi ga nakasawa na roba, kuma lokacin da aka buɗe ƙirar, waɗannan nakasar za su haifar da rikici tsakanin saman ƙarfe da ƙarfe. Idan rebound na roba yana da girma, zai kuma haifar da ƙarfin extrusion tsakanin robar da kuma mold surface, tilasta tsakiyar firam ya zama baka, da kuma roba abu ne extruded daga lankwasa frame kabu. A sakamakon haka, juriya na buɗewa yana ƙaruwa, yana haifar da wahala a rushewa, haifar da samfurin yaga, har ma da ƙura (yawanci samfurin yana da kayan skeleton karfe). Sabili da haka, ƙirar ƙira ya kamata a tabbatar da cewa sassan da aka ƙera suna da isasshen ƙarfi.

1.2.1.2 Juriya na juriya

Lokacin da samfurin ya rushe, ya zama dole don shawo kan juriya na buɗe ƙera da juriya na fitarwa. Mafi yawan lahani na ingancin samfurin da rashin kyawon kyallen ya haifar suna da alaƙa da wannan. Juriya na fitarwa ya fito ne daga riƙon ƙarfin samfurin zuwa ainihin, gami da ƙarfin da ke haifar da raguwa, extrusion, haɗin gwiwa da gogayya tsakanin saman robar da ƙarfe. Waɗannan sojojin ko dai suna ƙara ko kuma an haɗa su ta hanyoyi daban-daban don shafar sakin samfurin.

1.2.1.3 Tsarin fitarwa

The ejection inji kai tsaye rinjayar da ejection sakamako, da demoulding ejector sanda ne kullum shigar a cikin tsakiyar matsayi na mold, da kuma giciye-section yankin na demoulding ejector sanda kada ya zama ma kananan, domin ya hana wuce kima da karfi da naúrar yankin, yana da sauki don yin bakin ciki kayayyakin saman karya ko kayayyakin da karfe kwarangwal nakasawa. Lokacin samar da samfura tare da babban yanki da nauyi mai nauyi, don hana jujjuyawar wuce gona da iri da ke haifar da cunkoson aikin fitarwa ko lankwasa sandar ejector, ƙirar ƙirar yakamata a sanye ta da shingen jagorar rushewa na kusan ¢100mm, ko fiye da saita taron sandar ƙirar ƙira, amma yana buƙatar daidaitawa.

1.2.2 Tasirin masana'anta a kan sakin mold

A lokacin aikin masana'anta, ya kamata a bincika kogon, ƙwanƙwasa ƙwanƙwasa, da tazarar mating surface na tsarin sakawa, in ba haka ba zai shafi sakin samfurin. Ratar da ke tsakanin abin da aka saka da mating surface yana da girma sosai, roba yana da kaddarorin ruwa lokacin zafi, kuma roba yana da sauƙin matsewa yayin aiwatar da cikar ƙirƙira, yana haifar da walƙiya mai kauri, wanda ke hana ɓarna da bayyanar samfur. Bugu da ƙari, don samfuran bakin ciki mai zurfi mai zurfi, lokacin da aka fitar da su, an samar da vacuum a saman sashin da ainihin, yana haifar da wahala a rushewa. Sabili da haka, lokacin da aka ƙera ƙirar, ainihin ya kamata ya sami ramukan shan iska mai dacewa ko kuma ainihin farfajiyar ta kasance mai ƙaƙƙarfan (ba tare da rinjayar ingancin samfurin ba), wanda ya dace da saki.


1.3 Tasirin sigogin tsarin samarwa akan sakin mold

Siffofin tsarin samarwa suna da alaƙa da ingantattun lahani na samfuran, daga cikin abin da matsa lamba na allura, riƙe da matsa lamba, zafin vulcanization, abun ciki mai manne, lokacin ɓarna, da sauransu suna da babban tasiri akan rushewa. Lokacin da matsa lamba na allura ya yi yawa, zai haifar da nakasar sassa na gyaggyarawa kuma ya haifar da ƙarfin extrusion. Idan lokacin riƙewa ya yi tsayi da yawa, matsa lamba a cikin rami na ƙirƙira yana ƙaruwa, wanda zai haifar da ƙarfin juzu'i da damuwa na yanayin ƙwayoyin cuta. A lokaci guda kuma, ƙarfin alluran riƙe matsi yana da yawa kuma lokacin yana da tsayi sosai, wanda kuma zai haifar da cikawar tsari, haifar da babban damuwa na ciki, sannan kuma yana haifar da nakasar sassa ko walƙiya a tsakanin saman mating, wanda zai sa rushewar ta fi wahala. Vulcanization zafin jiki, roba abun ciki kudi, vulcanization lokaci suna da alaka da raguwar adadin roba, vulcanized roba abu ne mai sauki don samar da komawa zuwa ga asali sabon abu a high zafin jiki, babban shrinkage kudi na roba bayan vulcanization, mataimakin versa, kananan shrinkage. Mafi girman adadin abun ciki na roba, mafi girman raguwa, ƙananan abun ciki na roba, ƙarami ƙarami, mafi tsayin lokacin vulcanization, mafi girman darajar giciye, ƙaramin raguwa, ɗan gajeren lokacin vulcanization, ƙaramin lokaci na tsaka-tsakin lokaci, raguwar ƙima yana da girma, kuma raguwar raguwa yana da girma a cikin sharuddan ragewa ko raguwar aiki. per-vulcanization, kuma mafi ƙarancin raguwa yana da girma ne kawai a madaidaicin vulcanization, kuma riƙe da ƙarfi na mold tare da hadaddun cibiya da tsarin saka shi ma babba ne, wanda ba shi da amfani ga rushewar samfurin.


1.4 Tasirin hanyar aiki akan sakin mold

Wani nau'i na nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i nau'i) nau'i-nau'i-nau'i-nau'i-nau'i-nau'i-nau'i-nau'i-nau'i-nau'i-nau'i na yin amfani da kayan aiki iri ɗaya da kuma yin amfani da tsarin guda ɗaya, saboda ƙwarewar ma'aikata da hanyoyi daban-daban, sakamakon sakin da aka samu shima ya bambanta. Sabili da haka, ya zama dole a saba da kuma ƙware hanyar rushewar samfurin don samun sakamako mai kyau na rushewa. Anan ga wasu hanyoyin sakin ma'ana:

(1) Rushewar hannu yana ɗaya daga cikin hanyoyin samfuran roba don fitar da samfuran daga rami mai ƙura da ƙura, wanda ya dace da ƙananan sassa daban-daban da samfuran roba tare da babban tauri.

(2) Rushewar injina galibi ana amfani da shi don gyare-gyaren allura, gyare-gyaren simintin gyare-gyare da sauran manyan samfuran roba.

(3) Rushewar iska ita ce amfani da matsewar iska ko tafsirin tsotsawa don fitar da kayayyaki, babban fasalinsa shi ne: sauƙaƙa tsarin ƙirar, rage lokacin buɗewa da rufewa, rage ƙarfin aiki, da haɓaka haɓakar samarwa.

(4) Rushewar lalacewa shine yafi yin amfani da elasticity da kuma haɓaka mai kyau na roba, ta yin amfani da matsawa tilastawa ko lalatawar elongation, don samun sakamako mai lalacewa.

(5) Mold core demolding shine a buga ko danna maɓallin tsakiya lokacin rushewa, sa'an nan kuma buɗe mold ɗin don rushewa, wanda zai dace don tabbatar da ingancin samfurin da tasirin rushewa.

(6) Saka rushewa ya dace da ƙarin hadaddun ko samfura tare da abubuwan sakawa.


1.5 Tasirin gyare-gyaren ƙirƙira akan sakin mold

Ƙwararren nau'i-nau'i tare da tsari mai ma'ana, don tsawaita rayuwar sabis da tabbatar da ingancin samfurin, ban da amfani da hankali, ya kamata ku kula da kulawar ƙira. Bayan an yi amfani da mold, dole ne a duba abubuwan da ke gaba:

(1) Ko da mold ne maras kyau, musamman mold rami ko mold frame. Bayan da mold ya lalace, ba shi da amfani ga rushewar kayayyakin roba tare da kwarangwal na karfe ko babban taurin.

(2) Ko akwai sako-sako da jan gashi a bangaren da ake samu. Za a sami raguwa da alamomi lokacin da mold ya kwance kuma an ja shi, kuma bayan an matse kayan roba, yana da wuya a saki ƙirar, har ma da tsage samfurin.

(3) Ko matsayi abin dogaro ne. Gabaɗaya ana yin ramin ƙira ne daga samfuran samfuri da yawa waɗanda aka haɗa tare, kuma matsayar da ba daidai ba zai haifar da giɓi ko nakasar ƙirar.

(4) Ko saman mold rami ne santsi da kuma yadda shi ne m halin da ake ciki. Bayan tsatsa ko ɓarna ramin ƙura, za a haifar da babban juzu'i yayin aikin rushewar, wanda ba shi da amfani ga rushewar samfurin.

(5) Ko madaidaicin madaidaicin madaidaicin motsi da na'urorin haɗi a cikin ƙirar sun cika.

Idan akwai matsalolin da ke sama, ya kamata a gyara gyare-gyare, tsaftacewa, tsatsa, da dai sauransu.


2 Hattara

Abubuwan da ke sama suna nazarin tasirin abubuwa daban-daban akan rushewar samfuran, kuma suna gabatar da matakan da suka dace don kowane tasiri mai tasiri. Mahimman matakan don guje wa rashin kyawon kyallen takarda za a iya tafasa su zuwa:

(1) Tsarin samfurin yana da sauƙin rushewa, kuma yakamata a sami isassun gangaren rusa.

(2) Tsarin gyare-gyare yana da ma'ana, kuma an inganta ƙullun ƙirar kamar yadda zai yiwu.

(3) Daidaitacce ƙayyade sigogin tsarin samarwa.

(4) Inganta matakin aiki na ma'aikata.

(5) Kula da gyaran gyare-gyare.

(6) Rage gogayya kuma yi amfani da wakili mai sakin ƙura.

(7) Zaɓi dabarar ɗanko mai ma'ana kuma dacewa.


SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.