Kaddarori:
Matsanancin zafin jiki (-20 ° C zuwa + 250 ° C).
Musamman juriya ga mai, mai, kaushi, acid, da tushe.
Ƙarfin ƙarfi mai ƙarfi, ƙananan saitin matsawa, da kyakkyawan kwanciyar hankali na sinadarai.
Mai jure harshen wuta da kuma juriya na ozone.
Amfani:
Yana tsayayya da sinadarai masu tayar da hankali da yanayin matsa lamba.
Rayuwa mai tsawo a cikin sararin samaniya da aikace-aikacen mota.
Aikace-aikace:
Tsarin tsarin mai na jirgin sama, O-rings, da gaskets.
Hatimin watsa mota, bututun injin, da abubuwan turbocharger.
Sinadaran sarrafa kayan aikin rufi da gaskets.
Kaddarori:
Matsakaicin juriyar mai (fiye da roba na halitta amma ƙasa da FKM).
Mai hana wuta tare da kaddarorin kashe kai.
Kyakkyawan juriya na yanayi (UV, ozone, da danshi).
Mai sauƙi a ƙananan zafin jiki (-40 ° C zuwa + 120 ° C).
Amfani:
Cost-tasiri tare da sauƙin sarrafawa (extrusion / gyare-gyare).
Babban ƙarfin injiniya da juriya na abrasion.
Aikace-aikace:
Rigar rigar, safar hannu, da hoses na masana'antu.
Adhesives don takalma da gini.
Jaket ɗin igiyoyi da rufin rufin.
Kaddarori:
Ingantacciyar juriya mai zafi (har zuwa +150°C) idan aka kwatanta da NBR.
Mafi girman juriya ga mai, ruwan ruwa, da amines.
Ƙarfin ƙarfi mai ƙarfi da juriya ga gajiya.
Low permeability zuwa gases.
Amfani:
Yana riƙe da elasticity a ƙarƙashin tsayin daka zuwa ga sinadarai masu tsauri.
Tsawon rayuwa fiye da NBR a cikin matsanancin yanayi.
Aikace-aikace:
Kayan aikin hako mai da iskar gas (packers, likes).
Belin lokaci na mota, abubuwan allurar mai, da hatimin turbocharger.
Na'ura mai aiki da karfin ruwa cylinders.
Kaddarori:
Matsakaicin zafin jiki (-60°C zuwa +200°C).
Babban elasticity (har zuwa 1000% elongation).
Kyakkyawan rufin lantarki da kwanciyar hankali na thermal.
Biocompatible kuma inert.
Amfani:
Yana kiyaye sassauci a cikin yanayin cryogenic da yanayin zafi mai zafi.
Mai jure wa UV, ozone, da yanayin yanayi.
Aikace-aikace:
Na'urorin likitanci (catheters, implants).
Abubuwan lantarki (insulators, faifan maɓalli).
Gaskets masu zafi mai zafi don tanda da injuna.
Kaddarori:
Haɗa juriyar sinadarai ta FKM da sassaucin VMQ.
Yanayin zafin jiki: -50°C zuwa +230°C.
Mai juriya ga mai, man shafawa, da ruwan ruwa.
Ƙarƙashin matsawa saiti da kyakkyawan juriya.
Amfani:
Yana yin duka a cikin matsanancin zafi da ƙarancin zafi.
Mai jurewa kumburi a cikin makamashin jirgin sama.
Aikace-aikace:
Abubuwan da ke tattare da tsarin mai na jirgin sama (bawuloli, hatimi).
Gaskets da masu haɗawa mai zurfi-teku.
Na'urori masu auna motoci da tsarin sarrafa hayaki.
Kaddarori:
Fitaccen ozone da juriya na yanayi.
Babban ƙarfin dielectric da juriya na ruwa.
Yanayin zafin jiki: -50°C zuwa +150°C.
Rashin ƙarancin iskar gas.
Amfani:
Mafi tsada-tasiri don aikace-aikacen waje.
Kyakkyawan damping vibration da rage amo.
Aikace-aikace:
Motar yanayin yanayin mota, bututun radiyo, da hatimin iska.
Rufin rufin rufi da kandami liners.
Rufin kebul na lantarki da bel ɗin watsa wutar lantarki.