I. Vaaiga lautele o oloa pa'u fa'afefe

O oloa pa'u foam e gaosia ile faiga fa'afu'a fa'aletino po'o vaila'au fa'atasi ai ma le pa'u e fai ma mea fa'avae e maua mai ai mea fa'apipi'i pa'u pei ole omomi. O lenei tekinolosi ua faʻaaogaina lautele i fale gaosi oloa eseese, e pei o faitotoa o taavale ma faʻamaufaʻailoga faʻamalama, paʻu faʻapipiʻi, fale faufale faufale, mea faʻavevela, nofoaga puipuia o taʻaloga, ma isi.


1, Le manatu o foamed paʻu

O le mea e taʻua o le paʻu foamed e lauiloa tele foi o le paʻu paʻu tekonolosi, o le faʻaogaina lea o le faʻamaʻi faʻapitoa e togafitia ai le paʻu, ina ia maua ai e le paʻu se faʻatinoga faʻapitoa o se auala gaosi. O lenei tekinolosi e sili atu ona faʻaaogaina i le gaosiga o loʻo i ai nei, o le auala sili ona taatele o le gaosiga o galuega i lenei laasaga.


2, fa'avasegaina o oloa pa'u foamed

Foamed pa'u oloa i le taimi nei o se tasi o oloa sili ona faʻaaogaina i le gaosiga o fanua, lea e mafai ona vaevaeina i ni ituaiga se lua o microporous structure ma porous structure e tusa ai ma pores. Ma e mafai ona vaevaeina le fausaga microporous i oloa foaming eseese ma oloa foaming faifai pea. E tusa ai ma le mea mata o le paʻu e mafai ona vaevaeina i lenei oloa i le paʻu paʻu natura oloa faʻafefe, isoprene mea faʻafuga oloa, SBR foaming oloa, ethylene propylene rubber foaming oloa, ma isi.


Lona lua, oloa pa'u foam ma au'ili'iliga

Foamed oloa paʻu e sili atu ma sili atu ona faʻaaogaina i le sosaiete o loʻo i ai nei, o lona gaosiga ma le gaosiga o le gaosiga ma le thermoplastic foaming o loʻo i ai se lalolagi o le eseesega, o loʻo i ai se vulcanization cross-linking speed ma le saoasaoa o le decomposition o le foaming agent e fetaui ma le faafitauli. O lona uiga, o se mea paʻu manuia foaming i le faaopoopo atu i le saoasaoa o fesoʻotaʻiga o loʻo i ai se vavalalata vavalalata i le va o le vulcanization faagasologa o mea paʻu ma le decomposition o le sui feula e tupu pe a o le mataupu faavae e tutusa, o se faʻaopoopoga o le puipui faʻalautele kesi e maua ai le faagasologa tetee talafeagai.


1, Le filifiliga o mea autu

I le gaosiga o gaosiga, e masani ona manaʻomia le faʻamoemoega faʻapitoa o le oloa e filifili ai mea faʻasaienisi paʻu tino, o mea nei i le filifilia o le vaivai, malosi malosi, lelei le tele o le elasticity o oloa paʻu natura, ae ia filifili foi nisi paʻu faʻamalieina e fetaui ma manaʻoga o le oloa. Mo le gaosiga o oloa foam-tetee suauʻu, e faaopoopo atu i le manaomia e filifili se paʻu nitrile faasaienisi talafeagai, ae ia iloiloina foi le vaega ma le sootaga o le neoprene, ma e oo lava i le faamalieina o manaoga o nisi o oloa faapitoa, e mafai foi ona e faaaogaina le lua pe sili atu ituaiga o paʻu ma foliga.


2、O le filifiliga o le foaming sooupu

Foaming agent o le fesoʻotaʻiga sili ona taua i le gaosiga atoa o le paʻu foamed, ma o lona filifiliga e vavalalata vavalalata ma le lelei ma le lelei o le galuega. I se tulaga lautele, o le lelei o le faatinoga o le foaming oloa e tatau ona filifili se suʻesuʻega faʻasaienisi ma talafeagai, ma le aofaʻi o le foaming agent, le faʻaogaina o metotia e faʻafetaui ai manaʻoga o le atinaʻeina o agafesootai. I le taimi nei, o le sui feula e masani lava ona aofia ai soʻo faʻafefeteina ma soʻo faʻafefete lua. Inorganic feula sui e masani lava ona faasino i le sodium bicarbonate, ammonium bicarbonate, urea, ma isi. O nei sui feula o loʻo i ai le lelei o le saoasaoa decomposition vave ma le maualalo o le vevela i le talosaga, theoretically e sili atu foi lona faatinoga foaming. Talu ai o le kesi e gaosia e lenei tekinolosi i le talosaga e masani lava o le carbon dioxide ma le ammonia, ma isi mea, o le i ai o nei kasa e maua ai le fausaga o le paʻu e tele le faʻaogaina o le paʻu, e faigata ona faia se paʻu pupuni tapuni, o le gaosiga o le paʻu paʻu maualalo le lelei, maualalo le malosi, faʻafefe, faigofie ona faʻaleagaina, o lea e matua faigofie ai ona faʻaaogaina naʻo le faʻaogaina o le faʻaogaina o le faʻaaogaina o se mea faʻapitoa.

O le galuega o loʻo i ai nei, e masani ona matou faʻaaogaina le foaming agent e aofia ai le nitrogen dicarbonamide, nitroso, dibenzosulfonyl hydrazide ether, ma isi mea. e masani lava o loʻo i ai le nitrogen, carbon dioxide, ammonia, ma isi, o nei kasa e le gata e le oona, leai se manogi, ma e oʻo lava i le lelei o le le faʻaleagaina o le siosiomaga, e le o le lanu. O le tele o le pore o oloa pa'u pa'u e faia i le mea fa'afu'a e sili atu, ma o le fua fa'aitiitia e tele fo'i; pe a faʻaaogaina le mea faʻafefete, o le fesoasoani foaming agent o loʻo i ai le stearic acid, alum, ma isi mea, lea e mafai ona faʻaitiitia ai le vevela o le faʻafefe o le faʻafefe i le 130 ~ 150 ℃ pe a uma ona faʻaopopo.


3, le filifiliga o faiga vulcanization

Vulcanization faiga e taua tele i le faagasologa o suesuega o foaming oloa, muamua lava, pe o le fetaui o le faiga vulcanization ma faiga foaming o le ki i le faia lelei o le faatinoga o foaming oloa. O se paʻu e mafai ona manuia foamed, o le mea e sili ona taua o le vulcanization faagasologa o le paʻu ma le decomposition faagasologa o le foaming agent e tatau ona faavae synchronized, po o le sulfur taimi nai lo le taimi foaming teisi i luma. O le mea lea, a maeʻa ona filifilia le faiga faʻafefe, fetuunai le faiga faʻafefe e fetaui ma ia, pe a maeʻa ona filifilia le faiga faʻafefe, faʻafetaui le faiga faʻafefe e fetaui ma.


4, Le filifiliga o le faʻamalosia faʻatumu

O le carbon black, silica ma isi mea faʻamalosia e mafai ona faʻaleleia le malosi ma le faʻamalosi o oloa paʻu foamed, o le faʻaopoopoga talafeagai o le calcium carbonate, omea ma isi mea faʻatumu e mafai ona faʻaleleia ai le gaioiga o le paʻu ma faʻaitiitia le tau. Carbon uliuli e tatau ona filifili semi-faʻamalosia FEF ma SRF carbon uliuli, filler e tatau ona filifili malamalama calcium carbonate, omea, ma isi, le aofaiga e le tatau ona tele, sili 20 i 40 kopi.


5, Le filifiliga o plasticizer

O mea e mana'omia mo le Plasticizer e: lelei le palasitika, maualalo fua, vave absorption fua faatatau, fetaui lelei ma le pa'u, volatility laiti, leai migration, le oona, leai se manogi, taugofie ma faigofie ona maua. E mafai e le Plasticizer ona faʻaleleia le maualuga o le faʻasalalauina o le mea faʻapipiʻi, le faʻaogaina ma le faʻaogaina o le paʻu paʻu. O oloa pa'u foam e mana'omia ai le fa'ateleina foam maualuga, o le aofa'iga lautele o le plasticizer fa'aopoopo e sili atu, ma filifili se fetaui lelei ma le plasticizer pa'u.


6, Le filifiliga o le antioxidant

Fua pa'u oloa mo fausaga porous, o luga o le eria e tele, fai si faigofie i le matua, e tatau ona tuʻufaʻatasia ma antioxidants. O le mataupu faavae o le filifilia o le antioxidant e lelei uma le aoga anti-matua, ae e le afaina ai foi le pala o le foaming agent. E mafai ona filifili 4010, 264, MB ma isi antioxidants, le aofaʻi e sili atu nai lo oloa paʻu lautele.


7, le mataupu faavae o le paʻu foaming

Malosi paʻu foaming gaosiga o le omomi paʻu, o le mataupu faavae o le faaopoopo foaming sui sooupu i le paʻu filifilia po o le toe faaopoopo foaming sui sooupu, o le decomposition o le foaming sooupu i le vevela vulcanization e faamatuu atu le kesi, siomia e le paʻu e fausia ai se pu pupu 'ina ia le faalauteleina o le paʻu e fausia ai se omomi.

O mea autu e fuafua ma aʻafia ai le fausaga o le pore bubble o: o le aofaʻi o le sasaina o le kesi, le fua o le faʻasalalau o le kesi i totonu o le paʻu, o le viscosity o le paʻu ma le saoasaoa o le vulcanization, o le mea pito sili ona taua o le fetaui lea o le aofaʻi o le sasaina o le kesi, le saoasaoa o le gaosiga o le kesi ma le saoasaoa o le vulcanization o le paʻu.

Ina ia sili atu oloa pa'u, o le filifiliga o le feula le ituaiga o sui ma faiga vulcanization pa'u o le ki. E lua auala fa'apitoa:

Muamua, e tusa ai ma le vevela vulcanization e filifili le vevela pala ma le sui feula talafeagai, ma e tusa ai ma le saoasaoa decomposition o le sui feula i le vevela vulcanization e fetuutuunai le saoasaoa vulcanization o le paʻu, e pei o le faaaogaina o le tuai promoter ma isi faalauiloaina ma faiga vulcanization, e mafai ona faaaoga e fetuunai le aofaiga o le faalauiloaina e fetuunai le saoasaoa vulcanization.

Lona lua, i le tulaga o le faiga vulcanization e fuafua ai le saoasaoa o le vulcanization, e tusa ai ma le filifiliga o ituaiga foam ma talafeagai le tele o vaega. O le tele o le vaega o le mea e feula ai o se tasi lea o mea sili ona taua i le fuafuaina o le saoasaoa o le faʻaleagaina o le mea faʻafefe. E faʻaitiitia le tele o meaʻai, faʻateleina le vaega faʻapitoa o vaega, faʻateleina le faʻaleleia o le vevela, ma faʻavaveina le saoasaoa o le faʻaleagaina, o lea e mafai ai ona fetuunai le paleni i le va o le saoasaoa o le faʻafefeteina ma le saoasaoa o le vulcanization o le paʻu e ala i le filifilia o le vaega talafeagai o le feula.


Tolu, tekinolosi fa'agaioiga


1. Fa'apalapala

O le aano o le palasitika o pa'u mata o le talepe ma fa'aumatia le filifili macromolecular o pa'u. Faʻaleleia le palasitika o le paʻu, ina ia faigofie le faʻaogaina o le faʻafefiloi ma le faʻafefiloi o le mea faʻapipiʻi. I le sauniuniga o oloa pa'u foam, o le sili atu o le palasitika o le pa'u, o le faigofie foi lea o le faia o oloa e iai ni pu fa'aofuofu toniga, la'ititi la'ititi ma la'ititi laititi. O le mea lea, o le paʻu mata e tatau ona faʻapipiʻiina atoatoa.


2. Teuga

A maeʻa ona faʻafefiloi le paʻu, e tatau ona tuʻuina mo se taimi umi, e masani lava 2 ~ 4h, ina ia faʻasalalau atoatoa mea faʻaopoopo i totonu o le paʻu paʻu. O le sili atu le tutusa o mea faʻapipiʻi paʻu o loʻo faʻasalalau, o le sili atu lea o le mautu o le tele o oloa, o le lamolemole o luga ma le tutusa o pulu.


3, vevela

O le pulu paʻu e matua maaleale i le vevela. O le mea pa'u lava e tasi e eseese a'afiaga fa'afefe i le vevela eseese. Ona o le faiga foaming ma le faiga vulcanization e maaleale i le vevela eseese, suia le vevela vulcanization o le a toe fetuutuunai le faafitauli o le fetaui ma le faiga vulcanization ma le faiga foaming.


4. Fausiaina

O auala faʻapipiʻi o oloa paʻu foamed o: extrusion molding, molding, flat molding, ma isi EPDM foamed oloa e masani ona faʻaaogaina i le extrusion molding, ma le NBR e masani ona faʻaaogaina i le faʻaogaina.


SO'OGA VAIVAI

OA TATOU Oloa

FA'AALIGA FESOASOANI

Faʻaopoopo: Nu.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telefoni / WhatsApp / Skype: +86 15221953351
Puletaofia     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Faiga Fa'alilolilo | Lagolago e Leadong.