I. Ovaviu fɔ fom rɔba prodakt dɛn
Fɔm rɔba prodakt dɛn de prodyuz bay fizik ɔ kemikal fom we wit rɔba as di bays matirial fɔ gɛt spɔnj-layk rɔba porous strɔkchɔ prodakt. Dɛn dɔn yuz dis teknɔlɔji bɔku bɔku wan na difrɛn prodakshɔn industri dɛn, lɛk motoka domɔt ɛn winda sil, kusɛn pad, bildin kɔnstrɔkshɔn gasket, seismik matirial, spɔt protɛkshɔn fasiliti, ɛn ɔda tin dɛn.
1、Di kɔnsɛpt fɔ fom rɔba
Di tin we dɛn kɔl fom rɔba na tin we bɔku pipul dɛn sabi bak as rɔba fom teknɔlɔji, na di yus fɔ spɛshal fom ɛjɛn fɔ trit rɔba, so dat rɔba gɛt wan kwaliti pefɔmɛns fɔ wan prɔsesin we. Dis teknɔlɔji de yuz mɔ na di kɔrɛnt prodakshɔn fil, na di mɔs kɔmɔn we fɔ prodakshɔn wok na dis stej.
2、Klasifikeshɔn fɔ fom rɔba prodakt dɛn
Fɔm rɔba prodakt naw na wan pan di prɔdak dɛm we dɛn kin yuz mɔ na di prodakshɔn fil, we dɛn kin sheb to tu kayn maykroporous strɔkchɔ ɛn porous strɔkchɔ akɔdin to di pores. εn dεn kin sheb di maykroporous strכkchכ to sεparat fכm prodakt dεm εn kכntinyu fכm prodakt dεm. Akɔdin to di raw matirial fɔ rɔba dɛn kin sheb am to dis prɔdak to natura l rɔba fom prodak, isoprene fom prodak, SBR fom prodak, ethylene propylene rɔba fom prodak, ɛn ɔda tin dɛn.
Sɛkɔn, fom rɔba prodak wit analisis
Fɔm rɔba prodakt dɛn de yuz mɔ ɛn mɔ na di sosayti we de naw, in prodakshɔn ɛn prodakshɔn prɔses ɛn tɛmplastik fom gɛt wɔl difrɛns, i gɛt vulkanayzeshɔn krɔs-link spid ɛn di spid we di fom ɛjɛn de rɔtin fɔ mach di prɔblɛm. Dat min se, wan rɔba matirial saksesful fɔm in ad pan di krɔs-link spid de klos rilayshɔn bitwin di vulkanayzeshɔn prɔses fɔ rɔba matirial ɛn di dikɔmpɔzishɔn fɔ di blow ɛjɛn de apin we di prinsipul na basically di sem, na ɛkstenshɔn fɔ di gas ɛkspɛnshɔn wɔl fɔ prodyuz di kɔrɛspɔndɛns rɛsistɛns prɔses.
1、Di choice of di men matirial
Insay di manufakchurin prɔses, ɔltɛm nid di spɛshal ɔbjɛktiv dɛm fɔ di prɔdak fɔ pik di sayɛns rɔba bɔdi matirial dɛm, dɛn matirial ya insay di sɛlɛkshɔn fɔ sɔft, mɔdaret trɛnk, gud amɔnt fɔ ɛlastikiti fɔ natura rɔba prodak dɛm, bɔt bak fɔ pik sɔm atifishal rɔba fɔ mit di nid dɛm fɔ di prɔdak. Fɔ di prodakshɔn fɔ ɔyl-resistant fom prodak, apat frɔm di nid fɔ pik wan rizin sayɛns naytrayl rɔba, bɔt bak fɔ analayz di prɔpɔshɔn ɛn rilayshɔnship fɔ nioprene, ɛn ivin fɔ mit di nid fɔ sɔm spɛshal prɔdak, yu kin yuz tu ɔ mɔ kayn rɔba ɛn di fɔm bak.
2、Di choice of foaming ejen
Fom ejen na di link we impɔtant pas ɔl na di ɔl prodakshɔn fɔ fom rɔba, ɛn di we aw dɛn pik am gɛt fɔ du wit di efyushɔn ɛn kwaliti fɔ wok. Jɛnɛral wan, di gud pefɔmɛns fɔ di fom prodak dɛm fɔ pik wan sayɛns ɛn rizin fɔm ejen, ɛn di amount fɔ fom ejen, di yus ɔf we fɔ mit di soshal divɛlɔpmɛnt rikwaymɛnt dɛm we de naw. Naw, di blow ejen men wan gɛt ɔrganik blo ejen ɛn inɔrganik blo ejen tu. Inɔgɛnɛk blow ejen men wan de tɔk bɔt sɔdiɔm baykabɔnɛt, amɔniɔm baykabɔnɛt, yuria, ɛn ɔda tin dɛn. As di gas we dis teknɔlɔji de mek na di aplikeshɔn na men wan kabɔn dayɔgzayd ɛn amonia, ɛn ɔda tin dɛn, di prɛzɛns fɔ dɛn gas ya de mek di rɔba strɔkchɔ gɛt big permiabiliti kɔfishin, i at fɔ mek wan klos-ol fom rɔba, di prodakshɔn fɔ fom rɔba lɔw kwaliti, lɔw trɛnk, shrinkage, izi fɔ difɔmeshɔn, so i rili izi fɔ yuz in wan na di wok, ɛn jɔs lɛk ɔltin dɛn kin yuz am as ɔrganik foaming agent fɔ yuz.
Di wok we wi de du naw, wi kin yuz foaming ejen men wan gɛt naytrɔjen daykabɔnamid, naytroso, dibenzosulfonyl hydrazide ether, etc.. Dɛn matirial ya insay di aplikeshɔn fɔ in dikɔmpɔzishɔn tɛmpracha na lɛk 200 °C ɔ mɔ, ɛn insay di prodakshɔn prɔses nid bak fɔ ad ɔda ɔgzilari blow ejen, lɛk yuria, magnɛsiɔm ɔksayd, zink ɔksayd, ɛn ɔda tin dɛn.., so in dikɔmpɔzishɔn kin ridyus bad bad wan, di tɛmal dikɔmpɔzishɔn fɔ di gas we dɛn mek kin gɛt mɔ naytrɔjen, kabɔn dayɔgzayd, amonia, ɛn ɔda tin dɛn, dɛn gas ya nɔto jɔs nɔ pɔyzin, nɔ gɛt smel, ɛn ivin gɛt di bɛnifit fɔ nɔ dɔti di envayrɔmɛnt, nɔto fɔ chenj di kɔlɔ. di pore saiz fכ rכba fכm prodakt dεm we dεn mek wit fכm ejen big, εn di shrinkage rεt tu big; we yu de yuz fכm ejen, di כksijεn fכm ejen gεt stεarik asid, alum, εtk, we kin ridyus di dεkכmכshכn tεmprachכ fכ fכm ejen to 130~150°C afta dεn ad am.
3, di choice of vulcanization sistem
Vulcanization sistem rili impɔtant insay di risach prɔses fɔ fom prodak, fɔs, if di maching fɔ vulcanization sistem ɛn foaming sistem na di ki fɔ mek gud pefɔmɛns fɔ foaming prodak. Wan rɔba kin saksesful wan fɔm, di impɔtant tin na di vulkanayzeshɔn prɔses fɔ rɔba ɛn di dikɔmpɔzishɔn prɔses fɔ di fom ɛjɛn fɔ bi basically synchronized, ɔ sɔlfɔ tɛm pas di fom tɛm we de bifo smɔl. So, afta yu dɔn pik di vulkanayzeshɔn sistɛm, ajɔst di fɔm sistɛm fɔ mek i mach am, ɔ afta yu dɔn pik di fɔm sistɛm, ajɔst di vulkanayzeshɔn sistɛm fɔ mek i mach am.
4、Di chukchuk fɔ riinfɔs fila
Kabon blak, silika ɛn ɔda tin dɛn we de mek di rɔba strɔng kin mek di rɔba prodak dɛn we gɛt fom gɛt trɛnk ɛn stiff, if dɛn ad di rayt we fɔ ad kalsiɔm kabɔnɛt, kle ɛn ɔda tin dɛn we dɛn kin ful-ɔp, dat kin mek di rɔba wok fayn ɛn i kin mek di kɔst nɔ bɔku. Kabon blak fɔ pik sɛmi-riinfɔs FEF ɛn SRF kabɔn blak, fil fɔ pik layt kalsiɔm kabɔnɛt, kle, ɛn ɔda tin dɛn, di amɔnt nɔ fɔ tu bɔku, i bɛtɛ fɔ mek i bi 20 to 40 kɔpi.
5、Di choice fɔ plasticizayza
Di tin dɛn we dɛn nid fɔ mek plastizayza na: gud plasticizing effect, low dosage, fast absorption rate, gud kompitibiliti wit rɔba, smɔl volatility, nɔ maykreshɔn, nɔ pɔyzin, nɔ gɛt ɔda smel, i nɔ dia ɛn izi fɔ gɛt. Plastizayza kin impruv di digri we di kɔmpawnd ɛjɛn de skata, di prɔsesabiliti ɛn moldin fɔ di rɔba blɛnd. Fom rɔba prodak dɛm we nid ay fom multiplier, di jenɛral amɔnt fɔ plastizayza we dɛn ad big, ɛn pik wan gud kɔmpitibliti wit rɔba plastizayza.
6、Di chukchuk fɔ antiɔksidant
Fכm rכba prodakt fכ porous strכkchכ, sכfayz εria big, rili izi fכ ol, fכ kכmbayn wit antioksidant. di prinsipul fכ sεlekt antioksidant na כl tu gud anti-aging ifekt, bכt i nכ de afekt di dεkomposishכn fכ di fכm ejen. kin pik 4010, 264, MB ɛn ɔda antiɔksidant, di amɔnt we pas di jenɛral rɔba prodak dɛm.
7, di prinsipul fɔ mek rɔba fom
Sɔlid rɔba fom prodakshɔn fɔ rɔba spɔnj, di prinsipul na fɔ ad fom ejen insay di rɔba we yu dɔn pik ɔ ri-ad fom ejen, di dɛkɔmpɔzishɔn fɔ di fom ɛjɛn na di vulkanayzeshɔn tɛmpracha fɔ rilis gas, we dɛn rawnd wit rɔba fɔ mek wan bɔbul ol 'so dat di rɔba ɛkspɛnshɔn fɔ mek spɔnj.
di men tin dεm we de disayd εn infכlכ di strכkchכ fכ di bכbul pore na: di כmכnt כf di bכbul ejen gas, di gas difyushכn rεt insay di rכba, di viskositi fכ di rכba εn di spid we di vulkanizashכn de, di mכst krεs pan dεm na di mach fכ di כmכnt כf di bכbul ejen gas, di spid we di gas de jεnarεshכn εn di spid we di rכba de vulkanayz.
Fɔ mek bɛtɛ rɔba prodak, di chuk fɔ blo ejen spɛshal ɛn rɔba vulkanayzeshɔn sistɛm na di ki. Tu patikyula we dɛn de:
Fɔs, akɔdin to di vulkanayzeshɔn tɛmpracha fɔ pik di dikɔmpɔzishɔn tɛmpracha ɛn di aprɔpriet blow ejen, ɛn afta dat akɔdin to di dikɔmpɔzishɔn spid fɔ di blow ejen na di vulkanayzeshɔn tɛmpracha fɔ ajɔst di vulkanayzeshɔn spid fɔ di rɔba, lɛk fɔ yuz let prɔmota ɛn ɔda prɔmot ɛn vulkanayzeshɔn sistɛm, dɛn kin yuz fɔ ajɔst di amɔnt fɔ prɔmot fɔ ajɔst di vulkanayzeshɔn spid.
sεkכn, insay di kes fכ di vulkanayzεshכn sistεm fכ no di spid fכ vulkanayzεshכn, akɔdin to di chכys fכ fכm vεryut dεm εn di rayt patikyula saiz. Di patikyula saiz fɔ di ejen we de blo na wan pan di impɔtant tin dɛn bak fɔ no di spid we di ejen we de blo de pwɛl. di patikyula saiz de dכn, di spεsifi k sכfayz εria fכ di patikyula dεm de inkrεs, di hεt tכnfכs efyushכn de inkrεs, εn di dεkכmכshכn spid de aksεlεrayt, so di bεlε bitwin di dεkכmכshכn spid fכ di blכw ejen εn di vulkanayzεshכn spid fכ di rכba kin ajɔst bay we yu pik di fayn patikyula saiz fכ di blo ejen.
Tri, prɔsesin teknɔlɔji
1、Plastisayz we yu de yuz
Di men tin fɔ plasticiz raw rɔba na fɔ brok ɛn pwɛl di makromolikul chen fɔ rɔba. Impruv di plasticiti fɔ rɔba, so dat di miks ɛn blɛnd prɔses fɔ di kɔmpawnd ɛjɛn go izi fɔ du. We dɛn de pripia fɔm rɔba prɔdak, di mɔ di rɔba plasticiti bɛtɛ, na di mɔ i izi fɔ mek prɔdak dɛn we gɛt yunifom bɔbul ol, smɔl density ɛn smɔl shrinkage ret. So, di raw rɔba fɔ ful-ɔp wit plastic.
2、Stɔrej we dɛn de kip
afta dεn miks di rכba, dεn fכ put am fכ lכng inof tεm, jεnarali 2~4h, so dat difrεn aditiv dεm go fulכp skata insay di rכba miks. di mכr ivin di rכba aditiv dεm de skata, na di bεtεh di stεbiliti fכ di prodakt saiz, di smol smol sכfayz εn di yunifכm fכ di bכbul dεm.
3、Tɛmpratura
Rɔba fom kin rili sɛnsitiv to tɛmpracha. Di sem rɔba matirial gɛt difrɛn fom ifɛkt dɛn na difrɛn tɛmpracha. biכs di fכm sistεm εn di vulkanayzεshכn sistεm de sεnsitiv to tεmprachכ difrεnt, fכ chenj di vulkanayzεshכn tεmprachכ go rigεst di prכblεm fכ mach di vulkanayzεshכn sistεm wit di fכm sistεm.
4、Fɔm fɔm
Di we aw dɛn kin mol fɔm rɔba prɔdak na: ɛkstrushɔn moldin, moldin, flat moldin, ɛn ɔda tin dɛn.