ʻO ka hui ʻana o ka lāʻau ka mea e hoʻopuehu like ai i nā pūhui like ʻole me ke kōkua o ka ikaika mechanical o ka mīkini hana lāʻau, i mea e hana ai i ka multi-phase colloidal dispersion system me ka lāʻau ma ke ʻano he medium a i ʻole ka hui ʻana o ka lāʻau a me kekahi mau mea kūpono (matching agent, polymers ʻē aʻe) ma ke ʻano waena, a me nā mea hoʻohālikelike like ʻole (e like me ka pauka, zinc oxide, dispersed phase, etc.) kaʻina hana. ʻO nā koi ʻenehana kikoʻī o ke kaʻina hana hoʻohui ʻia: ʻo ka hoʻopuehu like ʻana o ka mea hoʻohuihui, no laila e hoʻokō ʻia ka hoʻopuehu maikaʻi loa o ka mea hoʻohuihui, ʻoi aku ka hoʻoikaika ʻana i ka mea hoʻohui e like me ke kalapona ʻeleʻele, e hōʻoia i ka hana mau ʻana o ka lāʻau. Kapa ʻia ka lāʻau hua i ka 'compounding rubber' a he mana koʻikoʻi kona maikaʻi i ka hana hou a me ka maikaʻi o ka huahana.
1 - Hoʻohui i ka neoprene
ʻO Neoprene nā ʻano emulsion polymerization o ka hana ʻana, ʻo ke kaʻina hana ka nui o ka polymerization intermittent kettle hoʻokahi. ʻO ka mahana o ka polymerization ka nui o ka mālama ʻia ma 40-60 ℃, a ʻo ka hoʻololi ʻana ma kahi o 90%. ʻO ka mahana polymerization, ʻoi aku ka kiʻekiʻe o ka hoʻololi hope loa a i ʻole ke kaʻina polymerization i ka lewa e alakaʻi i ka emi ʻana o ka maikaʻi o ka huahana. Hoʻoponopono ʻia ka nui molekala pili e ka ʻōnaehana sulfur-kiuram (tetraalkylmethylaminothiocarbonyldisulfide) i ka hana ʻana. ʻO ka hemahema nui o ka ʻōnaehana sulfur-kiuram, ʻo ia ka nele o ka paʻa o nā kaula sulfur, ʻo ia kekahi o nā kumu nui o nā waiwai mālama. Inā hoʻololi ʻia ka nui molekala pili me ka thiol hiki ke hoʻomaikaʻi i kēia hana. ʻOkoʻa ka Neoprene mai ka ʻōpala synthetic maʻamau, ʻaʻole ia e hoʻohana i ka vulcanization sulfur, akā me ka zinc oxide, magnesium oxide, etc. vulcanization.
ʻO ka hana ʻana o ka neoprene e pili ana i ka ʻano viscoelastic o ka lāʻau unvulcanized, a ʻo kāna ʻano viscoelastic e pili ana i ke ʻano o ka neoprene a me ka mahana. E like me ka hana maʻamau o ka hui ʻana ma ke kūlana elastic e hoʻohana i ka ikaika shear o ke kūlana elastic o ka ʻōpala e hoʻopuehu maikaʻi ai ka mea hoʻopihapiha. No laila, i mea e pale aku ai i ka hopena o ka wela kiʻekiʻe i ka hui ʻana i ka neoprene, pono e hoʻohui ʻia ka mea hoʻopiha i ka wā e hiki ai ke hoʻokō i kahi pae o ka hui ʻana i ke kūlana elastic. I ka hui ʻana me ka mea hoʻomaʻemaʻe hāmama, ua maʻalahi ka neoprene G-type i ka hoʻololi ʻana i ka mahana, a ʻoi aku ka mahana o ka ʻōwili ma mua o 70 ℃, e lilo ia i mau ʻōwili koʻikoʻi, a aia i loko o ke kahe kahe ʻana, a ʻaʻole maʻalahi ka hoʻopiha ʻana. I ka hui ʻana me kahi mea hoʻomaʻemaʻe paʻa, pono e hoʻemi ʻia kona hiki, kūpono ke kumu hoʻopiha piha o 0.6, maʻamau i hoʻokaʻawale ʻia i ʻelua hui ʻana, i mea e hōʻemi ai i ka wela o ka hui ʻana. Pono ka mahana hoʻokuʻu ma lalo o 100 ℃.
ʻO ka neoprene i ka hoʻohana ʻana i ka mīkini wehe ʻana i ka hui ʻana he nui ka wela, ʻoi aku ka maʻalahi o ka hoʻopili ʻana i nā wili, maʻalahi ke ʻā, me ka lohi o ka dispersion agent, no laila ʻaʻole kiʻekiʻe ke kiʻekiʻe o ka hui ʻana, liʻiliʻi ka hiki, ʻaʻole nui ka nui o ka wikiwiki. Ma muli o ka ikaika o ka naʻau i ka mahana, ka neoprene kumu nui i ka mahana o ka lumi a hiki i 71 ℃, e hōʻike ana ia i ka mokuʻāina, i kēia manawa ua nāwaliwali ka cohesion o ka ʻōpala maka, ʻaʻole wale nā roila koʻikoʻi koʻikoʻi, me ka hoʻopuehu ʻana o ka mea hana e paʻakikī loa. ʻO ka mahana wela o ka neoprene non-sulfur-regulated ma lalo o 79 ℃, no laila ʻoi aku ka maikaʻi o ke kaʻina hana hui ʻana ma mua o ka sulfur-regulated, a ʻoi aku ka liʻiliʻi o ka wili a me ka wela. ʻO ka hui ʻana me ka mīkini hāmama, i mea e pale aku ai i nā wili paʻa, e hoʻomalu ʻia ka wela o ka ʻōwili ma 40 ~ 50 ℃ a i ʻole (ʻo ka ʻōwili mua he 5 ~ 10 ℃ haʻahaʻa ma mua o ka wela o ka ʻōwili hope), a i ke kāwili ʻana i ka ʻōpala maka, pono e hoʻololi mālie ʻia ka mamao o ka ʻōwili mai ka nui a ka liʻiliʻi. I ka hui ʻana, e hoʻohui mua i ka magnesium oxide absorbent acid i mea e pale ai i ka ʻā, a i ka hope e hoʻohui i ka zinc oxide. I mea e hōʻemi ai i ka wela o ka hui ʻana, hiki ke hoʻohui ʻia nā ʻeleʻele kalapona a me nā mea hoʻoheheʻe wai i nā pūʻulu. Hiki ke hoʻopuehu liʻiliʻi ʻia ka ʻakika Stearic a me ka paraffin wax a me nā mea hana ʻē aʻe, i mea e kōkua ai i ka hoʻopuehu ʻana, akā no ka pale ʻana i nā wili paʻa. ʻO ka sulfur-regulated chloroprene rubber ma ka wehe ʻana i ka manawa hui ʻana he 30% a 50% ka lōʻihi ma mua o ka lāʻau kūlohelohe, hiki i ka 20% ka pōkole o ka manawa hui ʻole i hoʻoponopono ʻia ma mua o ka sulfur-regulated. I mea e pale aku ai i ka neoprene i loko o ka mīkini hui i ka wehe ʻana o ka piʻi ʻana o ka mahana me ka wikiwiki, ʻoi aku ka nui o ka wikiwiki ma mua o 1: 1.2 ma lalo, e ʻoi aku ka maikaʻi o ka hopena. ʻO ka hoʻohaʻahaʻa ʻana i ka hiki ke hoʻomaʻemaʻe he ala ia e hōʻoia ai i ka palekana o ka hana a me ka hoʻopuehu maikaʻi. I kēia manawa, ʻoi aku ka liʻiliʻi o ka sulfur-regulated neoprene rubber hoʻomaʻemaʻe ma mua o ka lāʻau maoli ma mua o 20% a 30%, i mea e hana maʻamau. E like me ka maʻalahi o ka neoprene i ka wela, no laila i ka hoʻohana ʻana i ka mīkini hoʻomaʻemaʻe nui e hoʻohana pinepine ʻia ka hui ʻana i ʻelua ʻano hui. Pono ka haʻahaʻa o ka hui ʻana (e hoʻomalu ʻia ka mahana hoʻokuʻu ʻana ma lalo o 100 ℃), ʻoi aku ka haʻahaʻa o ka hoʻouka ʻana ma mua o ka ʻōpala maoli (ʻo ka mea hiki ke lawe ʻia e like me 0.50 ~ 0.55), a hoʻohui ʻia ka zinc oxide i ka paʻi ma ka ʻāpana hui lua. No ka pilikia o ka hui ʻana o ka chloroprene he maʻalahi a paʻakikī hoʻi e hoʻopuehu, ua hoʻohana ʻo Leena Refiner i ka ʻehā apo pālua ʻehā e holo ana i ka ʻaoʻao hoʻokahi, i hui pū ʻia me ka neʻe ʻana o ka pihi 'X' o ka pahu kiʻekiʻe ma luna o ka mea hoʻomaʻemaʻe, me ka hopena dispersion maikaʻi a me ka manawa pōkole, hiki ke hōʻemi maikaʻi i ke kaʻina scorching o ke kaʻina chloroprene.
2 - Ka hui ʻana o ka ethylene propylene rubber
Hiki ke hoʻohana ʻia ka ethylene propylene rubber e nā mea hoʻomaʻemaʻe hoʻomaʻemaʻe maʻamau, akā no ka maikaʻi loa o ka hopena plasticizing o ka ethylene propylene rubber, ʻaʻole maʻalahi ka viscosity, ʻaʻole maʻalahi ka lāʻau e hoʻopili i ka ʻōwili, hoʻohana mua i ka pitch roll haiki, e hana i kahi pepa mau a laila e hoʻonui i ka pitch roll no ka hoʻopili ʻana i ka hana. ʻO ka mahana o ka'ōwili no ka'ōwili mua 50 ~ 60 ℃, ma hope o ka'ōwili 60 ~ 70 ℃ kūpono. ʻO ke kauoha hānai pāpaʻi EPDM ma ke ʻano maʻamau: ʻōwili uhi ʻōpala maka-1/2 kalapona ʻeleʻele-1/2 kalapona ʻeleʻele-stearic acid-zinc oxide (a i ʻole magnesium oxide) -promoter-crosslinker -Thin pass, lower sheet. ʻAʻole maʻalahi ka hoʻomaʻemaʻe ʻana o ka ethylene propylene rubber i ka wā e hui pū ai, a ua hoʻopuehu ʻia ka pūhui, akā ʻilihune ka waiwai paʻa ponoʻī. ʻO ka hui ʻana o ka ethylene-propylene rubber me ka mea hoʻomaʻemaʻe hāmama, e hoʻohana mua i kahi manawa ʻōwili liʻiliʻi e hoʻomau ai ma hope o ka ʻōwili, a laila hoʻomaha mālie i ka manawa ʻōwili, hoʻohui i ka pūhui, ka wela o ka ʻōwili ma waena o 60 ~ 70 ℃. ʻO ka mahana hui ʻana he 150 ~ 160 ℃, hiki ke kōkua i ka hoʻopuehu ʻana o ka hoʻopiha a me ka palupalu a me ka hoʻomaikaʻi ʻana i nā waiwai mechanical. Hiki i ka hoʻouka ʻana ke hiki ke 10% ~ 15% kiʻekiʻe ma mua o nā mea ʻē aʻe.
3- Ka hui pū ʻana o ka fluoroelastomer
ʻO ka fluorine rubber Menny viscosity he kiʻekiʻe, paʻakikī, hoʻomohala wela, ʻoi aku ka paʻakikī o ka hui ʻana a me ka hana ʻana. I ka hui ʻana i ka pulupulu fluorine ma ka mīkini hoʻomaʻemaʻe, i ka mamao o ka ʻōwili liʻiliʻi, ka liʻiliʻi o ka hiki, ka hoʻomalu ʻana i ka wela ma 50 ~ 60 ℃. Hoʻomaka ka hui ʻana, e hoʻomaʻamaʻa mua i nā wili, e hoʻohui i ka ʻōpala makaʻala ma kahi o 10 mau manawa e hana ai i kahi ʻāpana ʻōwili ʻōwili, hoʻoponopono i ka manawa o ka ʻōwili e mālama i kahi liʻiliʻi o ka pahu i hoʻopaʻa ʻia, a laila hoʻohui i ka mea hoʻohuihui, ʻaʻole maʻamau ka wehewehe ʻana i ka manawa hui, akā koi wikiwiki e like me ka hiki. ʻOi aku ka paʻakikī o ka fluorine rubber i ka hoʻohana ʻana i ka mīkini hui ʻana, akā ʻoi aku ka ikaika o ke ʻano meshing o ka mīkini hoʻoheheʻe ʻana i ka mīkini, hiki iā ʻoe ke hoʻohui i ka pulu fluorine. Pono e hoʻokuʻu ʻia ka lāʻau i hoʻohui ʻia no 24 mau hola ma mua o ka hoʻohana ʻana, a pono e hoʻomaʻemaʻe ʻia ma mua o ka hoʻohana ʻana i mea e hoʻopuehu like ʻia ai ka hui a hoʻomaikaʻi i ka wai a me ka paʻa ponoʻī o ka lāʻau.