Wɔde vinylidene fluoride (VDF) , hexafluoropropylene (HFP) ne tetrafluoroethylene (TFE) na ɛyɛ polymer akyi dompe no wɔ 40/30/30 nsusuwii a ɛyɛ pɛpɛɛpɛ mu, na ɛma wonya fluorine a ɛdɔɔso sen biara a ɛwɔ FKM a wɔtɔn mu . Saa fluorocarbon matrix a ɛyɛ den yi ma ahoɔden akwanside a ɛba fam koraa wɔ soro (< 18 mN m−1) a ɛpam hydrocarbons a ɛnyɛ polar , polar ester oils , ne nneɛma a wɔde ka ho denneennen te sɛ methanol anaa biodiesel. no Peroxide-scavenging bisphenol-AF cure nhyehyɛe yi brittle post-cure embrittlement fi hɔ, na ɛma > 20 MPa tensile ahoɔden ne 35 kN m−1 tear ahoɔden mpo wɔ 1,000 h @ 200 °C akyi . Nea afi mu aba ne aduru a ɛtra hɔ kyɛ sen silicone ne HNBR 3× wɔ ɔhyew envelope koro no ara mu bere a ɛkura < 3 % volume swell wɔ IRM903 reference oil mu.
| Agyapadeɛ | Sɔhwɛ Ɔkwan | FKM-65B20 Botaeɛ | Nnwuma Benchmark |
|---|---|---|---|
| Muduro | ASTM D792 na ɛwɔ hɔ | 1.82 g cm−3 na ɛwɔ hɔ | 1.80–1.85 na ɛwɔ hɔ |
| Hardness . | ASTM D2240 na ɛwɔ hɔ | 75 ± 3 Mpoano A | 70–80 na ɛwɔ hɔ |
| Ahoɔden a Wɔde Tensile | ASTM D412 na ɛwɔ hɔ | 20.5 MPa na ɛyɛ adwuma | > 18 MPa na ɛwɔ hɔ |
| Ntrɛwmu @ Break | ASTM D412 na ɛwɔ hɔ | 230 % . | > 180 % na ɛwɔ hɔ. |
| Nhyɛso Set (200 °C × 70 h) . | ASTM D395 na ɛwɔ hɔ | 18 % . | < 25 % . |
| Low-Temp Brittleness a Ɛyɛ Fɛ | ASTM D2137 na ɛwɔ hɔ | –25 °C na ɛwɔ hɔ | –20 °C na ɛwɔ hɔ |
| Volume Swell wɔ Petrol C (23 °C × 70 h) mu . | ASTM D471 na ɛwɔ hɔ | 1.2 % . | < 5 % . |
| Mpanyinyɛ wɔ Mframa mu 250 °C × 70 h | ASTM D573 na ɛwɔ hɔ | Nsakrae a ɛtwetwe nneɛma –5 % . | < –15 % . |
Turbocharger Nneɛma a Wɔde Yɛ Adwuma
Charge-air ducts ne blow-off valve diaphragms a wohu 260 °C peaks wɔ hard acceleration ase.
Wastegate actuator nsɔano a ɛko tia synthetic 5W-30 ngo + soot.
Fuel & SCR Nneɛma a Wɔde Yɛ Adwuma
Direct-injection O-rings a ɛkata 350 bar diesel pɛtro.
AdBlue (DEF) injector seals ano . a FKM-65B20 ’s low extractables siw crystallization efĩ
Engine & Nkrasɛm a Wɔde Kɔma
Oil cooler gaskets a wɔde ahyɛ 150 °C ngo + wosow mu.
E-motor dan grommets wɔ PHEVs a electrolyte vapors tow hyɛ standard elastomers.
Chassis & Breki a Wɔde Yɛ Nneɛma
ESP hydraulic accumulator bladders a ɛhia < 0.1 % pɛtro a ɛkɔ mu.
Mframa a ɛsensɛn hɔ a ɛko tia ozone, kwan so nkyene, ne breki nsu.
Compound Form : wɔadi kan afra Slab, strip, anaa pellet a a wɔasiesie ama compression, transfer, anaa injection molding.
Typical Cure Cycle : 5 min @ 170 °C press + aduru akyi 2 h @ 200 °C (mframa) anaa 30 min @ 230 °C nsuo a ɛyɛ hyew ma < 1 % extractables.
Slab Nsusuwii : 300 mm × 300 mm × 10 mm (a wɔahyɛ da ayɛ 2–30 mm).
Shelf Life : Asram 12 @ ≤ 25 °C wɔ aluminium-foil/PE bag abien mu; wɔde nitrogen afra mu na amma oxidative scorch ankɔ.
ISO 9001:2015 & IATF 16949:2016 adansedie krataa a wɔde yɛ adwuma.
REACH & RoHS 3.0 mpaemuka a edi mũ (SVHC < 0.1 %).
SGS Sɔhwɛ Amanneɛbɔ – tetew, nhyɛso set, pɛtro a ɛho ahonhon (twe PDF).
Ntawntawdi mu Aboɔden abo ho asɛm – DRC-free sourcing.
| Order Type | MOQ | Bere a edi kan | a wɔde kyekyere nneɛma | Incoterm |
|---|---|---|---|---|
| Stock Compound a Wɔde Yɛ Nneɛma | 25 kg | nnafua 7–10 | PE bag + krataa a wɔde yɛ adwuma | EXW Shenzhen na ɔkyerɛwee |
| Amanne Kɔla/Hardness | 250 kg na ɛyɛ | Adapɛn 3–4 | Wɔde vacuum ahyɛ mu | FOB Shenzhen na ɔkyerɛwee |
| Wɔayɛ no pelletized ama Extrusion | 500 kg | Adapɛn 4–5 | 25 kg a wɔde ayɛ nkotoku a wɔde foil ayɛ | CIF Hamburg na ɔkyerɛwee |
Bundle with Stainless-Steel Cable Ties
Sɛ turbocharger harnesses a ɛda adi > 200 °C , fa FKM-65B20 gaskets ne yɛn 316 SS cable ties rated –80 °C kosi +538 °C ma thermal-chemical sealing nhyehyɛe a edi mũ.