HNBR Rubber a Ɛyɛ Ahoɔden a Ɛko Tia Ngo a Ɛyɛ Medium-Saturation
Product Overview: High-Strength Oil-Resistant Medium-Saturation HNBR Synthetic Rubber
Wɔayɛ yɛn Medium-Saturation HNBR Synthetic Rubber no sɛnea ɛbɛyɛ a ɛde adwumayɛ soronko bɛma wɔ mfiridwuma mu mmeae a ngo a ɛda adi ne adwennwen kɛse wom. Esiane sɛ acrylonitrile 34% na ɛwɔ mu nti, saa hydrogenated nitrile rubber (HNBR) yi ma ngo a ɛko tia yiye bere a ɛma ɛyɛ mmerɛw na ɛtra hɔ kyɛ, na ɛma ɛyɛ nea eye ma nsɔano, gasket, ne nneɛma a ɛwom wɔ adwumayɛ tebea a emu yɛ den mu.
Mfiridwuma ho nsɛm titiriw:
- Acrylonitrile Nneɛma a ɛwɔ mu: 34% – Wɔayɛ no yiye ama ngo a ɛkari pɛ a ɛko tia ne ɔhyew a ɛba fam a ɛyɛ mmerɛw.
- Mooney Viscosity (ML 1+4 @125°C): 70-90 – Ɛhwɛ hu sɛ ɛyɛ adwuma yiye ma nkuku ne extrusion.
- Iodine Absorption Value: 11-22 – Ɛda controlled medium saturation adi ma nnuru a ɛyɛ den ne onyin a ɛko tia.
- Hardness: Adjustable range (sɛ nhwɛsoɔ, 60-90 Shore A) de di dwumadie ahodoɔ ahwehwɛdeɛ ho dwuma.