Umugongo wa polymer wubatswe muri floride ya vinylidene (VDF) , hexafluoropropylene (HFP) na tetrafluoroethylene (TFE) ku kigereranyo cya 40/30/30, itanga florine nyinshi iboneka muri FKM yubucuruzi . Iyi matrike yuzuye ya fluorocarubone ikora inzitizi zidasanzwe zubutaka (<18 mN m⁻¹) zisubiza inyuma ya hydrocarbone ya polar estar , amavuta , hamwe ninyongeramusaruro nka methanol cyangwa biodiesel. Sisitemu yo gukiza perpxyde-bisphenol-AF ikuraho uburyo bworoshye bwo gukira nyuma yo gukira, bigatanga > 20 MPa imbaraga zingana na 35 kN m⁻¹ amarira na nyuma ya 1.000 h @ 200 ° C. Igisubizo nikintu kibaho silicone na HNBR kuri 3 × mu ibahasha imwe yubushyuhe mugihe ukomeza <3% kubyimba mumavuta ya IRM903.
| Umutungo | Uburyo bwo Kugerageza | FKM-65B20 Agaciro Agaciro | Inganda |
|---|---|---|---|
| Ubucucike | ASTM D792 | 1.82 g cm⁻³ | 1.80–1.85 |
| Gukomera | ASTM D2240 | 75 ± 3 Inkombe A. | 70-80 |
| Imbaraga | ASTM D412 | 20.5 MPa | > 18 MPa |
| Kurambura @ Kuruhuka | ASTM D412 | 230% | > 180% |
| Gushiraho (200 ° C × 70 h) | ASTM D395 | 18% | <25% |
| Ubushyuhe buke | ASTM D2137 | –25 ° C. | –20 ° C. |
| Umubyimba mwinshi muri lisansi C (23 ° C × 70 h) | ASTM D471 | 1,2% | <5% |
| Gusaza mu kirere 250 ° C × 70 h | ASTM D573 | Impinduka zingana –5% | <–15% |
Sisitemu ya Turbocharger
Imiyoboro yo mu kirere hamwe na diafragma ya valve ibona impinga ya 260 ° C yihuta cyane.
Ikirangantego cya Wastegate kirwanya amavuta ya 5W-30 amavuta + soot.
Ibicanwa na SCR
Gutera inshinge O-impeta zifunga amavuta ya mazutu 350.
Ikidodo cya AdBlue (DEF) kashe aho FKM-65B20 ikuramo ibintu bike birinda kristu.
Moteri & Kohereza
Amavuta akonje ya peteroli yerekanwe na 150 ° C amavuta + kunyeganyega.
E-moteri yimyubakire yibikoresho muri PHEV aho imyuka ya electrolyte yibasira elastomers isanzwe.
Chassis & Feri
ESP hydraulic yegeranya uruhago ikenera <0.1% ya peteroli.
Umuyaga uhagarika ikirere urwanya ozone, umunyu wo mumuhanda, hamwe na feri ya feri.
Ifumbire mvaruganda : Mbere yo kuvanga icyapa, umurongo, cyangwa pellet yiteguye guhonyora, kwimura, cyangwa guterwa inshinge.
Inzira isanzwe yo gukira : 5 min @ 170 ° C kanda + nyuma yo gukira 2 h @ 200 ° C (umwuka) cyangwa 30 min @ 230 ° C icyuka kuri <1% ikuramo.
Ibipimo by'icyapa : 300 mm × 300 mm × 10 mm (gakondo 2-30 mm).
Ubuzima bwa Shelf : amezi 12 @ ≤ 25 ° C muri aluminium-foil / PE igikapu kabiri; azote-isukuye kugirango irinde okiside.
ISO 9001: 2015 & IATF 16949: 2016 igihingwa cyemewe.
REACH & RoHS 3.0 imenyekanisha ryuzuye (SVHC <0.1%).
Raporo y'Ikizamini cya SGS - amarira, gushiraho compression, kubyimba lisansi (gukuramo PDF).
Amabuye y'agaciro avuguruzanya - DRC itagira isoko.
| Ubwoko | MOQ | Iyobora Igihe | Gupakira | Incoterm |
|---|---|---|---|---|
| Ikigega cyimigabane | 25 kg | Iminsi 7-10 | PE igikapu + ikarito | EXW Shenzhen |
| Ibara ryihariye / Gukomera | 250 kg | Ibyumweru 3-4 | Ikibanza gifunze icyuho | FOB Shenzhen |
| Pelletised for Extrusion | 500 kg | Ibyumweru 4-5 | 25 kg imifuka | CIF Hamburg |
Bundike hamwe na kabili ya kaburimbo idafite ibyuma
Kubikoresho bya turbocharger byerekanwe na > 200 ° C , guhuza gaseke ya FKM-65B20 hamwe na kabili ya 316 SS ya kabili yashyizwe kuri 80 ° C kugeza kuri + 538 ° C kugirango sisitemu yuzuye yo gufunga amashyuza-shimi..