FKM-65B20
| Muaj: | |
|---|---|
| Quantity: | |
Cov pob txha polymer yog tsim los ntawm vinylidene fluoride (VDF) , hexafluoropropylene (HFP) thiab tetrafluoroethylene (TFE) nyob rau hauv ib tug meej 40/30/30 piv, yielding siab tshaj plaws fluorine cov ntsiab lus muaj nyob rau hauv ib tug coj mus muag FKM . This dense fluorocarbon matrix creates an ultra-low surface energy barrier (< 18 mN m⁻¹) that repels non-polar hydrocarbons , polar ester oils , and aggressive additives such as methanol or biodiesel. Lub peroxide-scavenging bisphenol-AF kho system tshem tawm nkig tom qab kho embrittlement, muab > 20 MPa tensile lub zog thiab 35 kN m⁻¹ tsim kua muag zog txawm tias tom qab 1,000 h @ 200 ° C. Qhov tshwm sim yog qhov sib xyaw ua ke uas tawm ntawm silicone thiab HNBR los ntawm 3 × hauv tib lub hnab ntawv thermal thaum tuav <3% ntim o hauv IRM903 siv roj.
| Cov Khoom | Txoj Kev Ntsuas | FKM-65B20 Tus Nqi | Kev Lag Luam |
|---|---|---|---|
| Qhov ntom | ASTM D 792 Cov Lus Qhia Tshwj Xeeb | 1,82 g cm | 1.80–1.85 Nws |
| Hardness | ASTM D 2240 Cov Lus Qhia | 75 ± 3 Ntug A | 70–80 : kuv |
| Tensile zog | ASTM D412 | 20.5 MPa | > 18 MPa |
| Elongation @ Sib | ASTM D412 | 230% | > 180% |
| Compression Teeb (200 ° C × 70 h) | ASTM D 395 Cov Lus Qhia | 18% | <25% |
| Low-Temp Brittleness | ASTM D 2137 Cov khoom lag luam | -25 ° C | -20 ° C |
| Volume Swell hauv Roj C (23 ° C × 70 h) | ASTM D 471 Cov Lus Qhia | 1.2% | <5% |
| Kev laus hauv Cua 250 ° C × 70 h | ASTM D 573 3 | Tensile hloov - 5% | <-15% |
Turbocharger Systems
Charge-air ducts thiab blow-off valve diaphragms uas pom 260 ° C peaks nyob rau hauv lub zog acceleration.
Wastegate actuator seals tiv thaiv hluavtaws 5W-30 roj + soot.
Roj & SCR Circuits
Direct-injection O-rings sealing 350 bar diesel roj.
AdBlue (DEF) injector seals qhov twg FKM-65B20 's low extractables tiv thaiv crystallization fouling.
Cav & Kis
Roj txias gaskets raug rau 150 ° C roj + kev co.
E-motor Housing grommets in PHEVs where electrolyte vapors attack standard elastomers.
Chassis & Brakes
ESP hydraulic accumulator zais zis xav tau <0.1% roj permeation.
Lub tshuab nqus tsev twj tso kua mis tiv thaiv ozone, txoj kev ntsev, thiab cov dej nres.
Compound Form : Pre-mixed slab, sawb, los yog pellet npaj rau compression, hloov, los yog txhaj tshuaj molding.
Kev Kho Mob Cycle : 5 min @ 170 ° C xovxwm + tom qab kho 2 h @ 200 ° C (cua) los yog 30 min @ 230 ° C chav rau <1% extractables.
Slab Dimensions : 300 mm × 300 mm × 10 mm (kev cai 2-30 mm).
Lub neej txee : 12 lub hlis @ ≤ 25 ° C hauv aluminium-foil / PE ob lub hnab; nitrogen-flushed los tiv thaiv oxidative scorch.
ISO 9001: 2015 & IATF 16949: 2016 certified compounding nroj tsuag.
REACH & RoHS 3.0 daim ntawv tshaj tawm tag nrho (SVHC <0.1%).
SGS Test Report - kua muag, compression set, roj swell (download PDF).
Cov Lus Qhia Tsis Pom Zoo - DRC-dawb qhov chaw.
| Order Type | MOQ | Lead Time | Packaging | Incoterm |
|---|---|---|---|---|
| Stock Compound | 25 kg ib | 7-10 hnub | PE hnab + thawv | EXW Shenzhen |
| Kev cai xim / Hardness | 250 kg | 3-4 lub lis piam | Nqus-sealed strip | FOB Shenzhen |
| Pelletized rau Extrusion | 500 kg | 4-5 lub lis piam | 25 kg foil hnab | CIF Hamburg |
Bundle nrog Stainless-Steel Cable Ties
Rau turbocharger harnesses raug > 200 ° C , khub FKM-65B20 gaskets nrog peb 316 SS cable ties ntsuas -80 ° C rau + 538 ° C rau ua tiav thermal-chemical sealing system.