di polimכr bakbon dεn bil am frכm vinyliden fluoride (VDF) , hexafluoropropylene (HFP) εn tetrafluoroethylene (TFE) insay wan prεsis 40/30/30 rεshכ, we de gi di hεyest fluorine kכntεnt we de insay wan kכmεshכnal FKM . Dis dense fluorocarbon matris de mek wan ultra-low surface enaji barɛri (< 18 mN m−1) we de ripel non-polar hydrocarbons , polar ester oils , ɛn agresiv aditiv dɛm lɛk mɛtanɔl ɔ bayɔdizil. di pεrכksayd-skavεnj bisfεnol-AF kכryu sistεm de εliminet britl pכst-kכyr εmbritεlmεnt, we de gi > 20 MPa tεnsil strכng εn 35 kN m−1 tεar strכng ivin afta 1,000 h @ 200 °C . di rizulεt na wan kכmpawnd we de liv pas silikon εn HNBR bay 3× insay di sem tεmral εnvεlop we i de mεnten < 3 % vכlyum swεl insay IRM903 rεfrεns כyl.
| Prɔpati | Tɛst Mɛtɔd | FKM-65B20 Valyu | Indastri Bɛnchmak |
|---|---|---|---|
| Tik | ASTM D792 we yu de yuz | 1,82 g cm−3 | 1.80–1.85 |
| Di at we pɔsin kin gɛt | ASTM D2240 we yu de yuz | 75 ± 3 Shor A. | 70–80 |
| Tensile Strɔng we pɔsin kin gɛt | ASTM D412 we yu kin yuz | 20.5 MPa | > 18 MPa we yu de yuz |
| Elongation @ Brek we yu de du | ASTM D412 we yu kin yuz | 230 % . | > 180 % na di . |
| Set kompresi (200 °C × 70 h) . | ASTM D395 we de na di wɔl | 18 % . | < 25 % . |
| Lɔw-Tɛmp Britlɛshɔn | ASTM D2137 we yu de yuz | –25 °C na di wɔl | –20 °C we yu de du |
| Volyum Swɛl insay Fiul C (23 °C × 70 h) . | ASTM D471 we yu kin yuz | 1.2 % . | < 5 % . |
| Aging in Eriya 250 °C × 70 h | ASTM D573 we yu kin yuz | Tensile chenj –5 % . | < –15 % ɛn di ɔda wan dɛn. |
Turbocharger Sistem dɛn we dɛn kin yuz
Chaj-ɛya dakt ɛn blo-ɔf valv dayafragm dɛn we de si 260 °C pik dɛn ɔnda had aksilarayshɔn.
Wastegate aktyuator sil dɛn we de rɛsist sintetik 5W-30 ɔyl + sɔt.
Fiul & SCR Sakit dɛn
Dairekt-injɛkshɔn O-ring dɛn we de sial 350 bar dizil fiul.
AdBlue (DEF) injekta sil usay FKM-65B20 ’s lɔw ɛkstraktabl dɛn de mek kristalizayshɔn fɔul nɔ de.
Enjin & Transmishɔn
Oil kul gasket dεm we dεn εkspos to 150 °C כyl + vaybrεshכn.
E-motor hausing grommets in PHEVs usay ilektrolayt vapours atak standad elastomers.
Chasis & Brek dɛn
ESP haydrolik akumulatɔ blad dɛn we nid < 0.1 % fiul pɔrmieshɔn.
Ɛya-sɔspɛns bɛlɔ dɛn we nɔ de mek di ɔzoyn, rod sɔl, ɛn brek fluid nɔ kam.
Kɔmpawnd Fɔm : Prɛ-miks slab, strip, ɔ pɛlɛt we rɛdi fɔ kɔmpreshɔn, transfa, ɔ injɛkshɔn mold.
Tipik Kכr Saykl : 5 min @ 170 °C prεs + pכst-kכr 2 h @ 200 °C (εya) כ 30 min @ 230 °C stim fכ < 1 % εkstraktabl.
Slab Dimenshɔn : 300 mm × 300 mm × 10 mm (kɔstɔm 2–30 mm).
Shelf Layf : 12 mɔnt @ ≤ 25 °C insay aluminiɔm-fɔyl/PE dɛbul bag; naytrɔjen-flɔsh fɔ mek di ɔksidativ skɔch nɔ apin.
ISO 9001:2015 & IATF 16949:2016 sɛtifiket kɔmpawnd plant.
REACH & RoHS 3.0 ful diklareshɔn (SVHC < 0.1 %).
SGS Test Ripɔt – tear, kɔmpreshɔn sɛt, fiul swel (dawlod PDF).
Kɔnflikt Minral Stetmɛnt – DRC-fri sɔs.
| Ɔda Tayp | MOQ | Lid Taym | Pakɛj | Incoterm |
|---|---|---|---|---|
| Stok Kɔmpawnd | 25 kg | 7–10 dez | PE bag + katon we dɛn kin yuz | EXW Shenzhen we de wok fɔ di kɔmni |
| Kastom Kɔlɔ/Hadnɛs | 250 kg | 3–4 wiks | Strip we dɛn dɔn sidɔm wit vaykum | FOB Shenzhen, we de na di wɔl |
| Pɛlɛtayz fɔ Ɛkstrushɔn | 500 kg | 4–5 wiks | 25 kg foil bags | CIF Hamburg |
Bundle wit Stainless-Steel Cable Ties
Fɔ turbocharger harnesses we dɛn dɔn ɛkspos to > 200 °C , pe FKM-65B20 gaskets wit wi 316 SS kebul tays we dɛn rayt –80 °C to +538 °C fɔ wan kɔmplit thermal-chemical siling system.