Amavuta-Imbaraga-Zirwanya Hagati-Yuzuye HNBR Rubber Synthetic Rubber
Incamake y'ibicuruzwa: Imbaraga-nyinshi-Amavuta-Kurwanya Hagati-Kwiyuzuzamo HNBR Rubber Synthetic
Rubber Hagati-Yuzuye HNBR Synthetic Rubber yakozwe kugirango itange umusaruro udasanzwe mubikorwa byamavuta yibasiwe n’inganda. Hamwe na 34% bya acrylonitrile, iyi hydrogène nitrile reberi (HNBR) itanga amavuta arwanya imbaraga mugihe ikomeza guhinduka kandi ikaramba, bigatuma iba nziza kuri kashe, gasketi, nibigize iri kashe, gasketi, nibigize ibintu bguhinduka kandi ikaramba, bigatuma iba nziza kuri kashe, gasketi, nibigize ibintu bikora nabi.
Ibyingenzi bya tekinike Ibisobanuro:
- Ibirimo Acrylonitrile: 34% - Gukoresha uburyo bwiza bwo kurwanya amavuta hamwe nubushyuhe buke.
- Ubukonje bwa Mooney (ML 1 + 4 @ 125 ° C): 70-90 - Iremeza uburyo bwiza bwo gutunganya no gusohora.
- Agaciro ka Iyode Agaciro: 11-22 - Yerekana ubwuzuzanye buciriritse bugamije kongera imiti no kurwanya gusaza.
- Gukomera: Urwego ruhinduka (urugero, 60-90 Inkombe A) kugirango uhuze ibyifuzo bitandukanye.