Hydrogenated nitrile roj hmab precompound thiab compound-HNBR
Hydrogenated nitrile roj hmab (HNBR los yog HSN) yog cov khoom ntawm hydrogenation thiab saturation ntawm carbon-carbon ob daim ntawv cog lus nyob rau hauv lub molecular saw ntawm nitrile roj hmab, yog li nws kuj hu ua heev saturated nitrile roj hmab.
HNBR muaj cov roj ua haujlwm zoo (ua haujlwm zoo rau roj roj, lubricants, cov kuab tshuaj tsw qab); thiab vim nws cov qauv saturated heev, nws muaj cov cua kub zoo, cov tshuaj tiv thaiv zoo heev (zoo tsis kam rau Freon, acids thiab alkalis), ozone kuj zoo heev, thiab siab tsis kam mus tas li deformation hauv compression; tib lub sijhawm, HNBR kuj muaj lub zog siab, siab tearing kev ua tau zoo. HNBR kuj muaj lub zog siab, siab ua kua muag, zoo heev hnav tsis kam, thiab lwm yam. Nws yog ib qho ntawm cov roj hmab nrog kev ua tau zoo tag nrho.
Herchy Rubber muaj pab pawg kws tshaj lij nrog kev paub dhau los hauv HNBR R & D. Peb tuaj yeem tsim cov khoom siv sib txawv raws li cov neeg siv khoom xav tau. Thiab txaus siab rau lub koob npe nrov hauv Suav teb thiab thoob ntiaj teb.
| Herchy | Vulcanization hom | Cov ntsiab lus ntawm Acrylonitrile | Mooney viscosity | Hardness | Tensile zog | Elongation thaum so | IRM 903 Volume hloov pauv | Compression teeb | Daim ntawv thov | Cim |
| 150 ℃ * 72 h | 150 ℃ * 72h ASTM D395 Hom B | |||||||||
| Qib | % | ML (1 + 4) 100 ℃ | Ntug A | Mpa | % | % | % | |||
| HNBR-S6035 | Sulfur | 35 | 50 ~ 100 | 60 | 17-24 : kuv | 300-500 | <20 | <60 | Cov khoom hauv oilfield kev lag luam, | Zoo elongation, Zoo self-adhesiveness, Exllent ua |
| HNBR-S7035 | Sulfur | 35 | 50 ~ 100 | 70 | 17-24 : kuv | 300-500 | <20 | <60 | Cov khoom lag luam hauv oilfield kev lag luam, Tsheb lag luam, Siv |
Dynamic qaug zog tsis kam, Zoo tus kheej-Resistance, Exllent ua |
| HNBR-S8035 | Sulfur | 35 | 50 ~ 100 | 80 | 17-24 : kuv | 300-500 | <20 | <60 | Drilling yeeb nkab tiv thaiv txheej, Pwm accumulators |
Kev kub siab tsis kam, Zoo tus kheej-adhesiveness |
| HNBR-S6043 | Sulfur | 43 | 50 ~ 100 | 60 | 17-24 : kuv | 300-500 | <10 | <60 | Tsheb roj, Cov khoom hauv oilfield kev lag luam |
Roj kuj, Exllent ua |
| HNBR-S7043 | Sulfur | 43 | 50 ~ 100 | 70 | 17-24 : kuv | 300-500 | <10 | <60 | Cov khoom lag luam hauv oilfield kev lag luam, Tsheb lag luam, |
Roj kuj, Dynamic qaug zog tsis kam, Zoo tus kheej ua haujlwm |
| HNBR-S8043 | Sulfur | 43 | 50 ~ 100 | 80 | 17-24 : kuv | 300-500 | <10 | <60 | Drilling yeeb nkab tiv thaiv txheej, Pwm accumulators |
Roj tsis kam, Siab siab tsis kam, Zoo tus kheej-adhesiveness |
| HNBR-P6035 | Peroxide | 35 | 50 ~ 100 | 60 | 17-24 : kuv | 200-350 | <20 | <30 | Automotive kev lag luam, Aircraft manufacturing kev lag luam |
High tempreture kuj, Exllent ua |
| HNBR-P7035 | Peroxide | 35 | 50 ~ 100 | 70 | 17-24 : kuv | 200-350 | <20 | <30 | Kev tsim kho kev lag luam, Cav gaskets, O-rings, Seals |
High tempreture kuj, Zoo compression teeb |
| HNBR-P8035 | Peroxide | 35 | 50 ~ 100 | 80 | 17-24 : kuv | 200-350 | <20 | <30 | Drilling kav, Siab accumulators, |
Kev kub siab tsis kam, Siab tempreture kuj |
| HNBR-P6043 | Peroxide | 43 | 50 ~ 100 | 60 | 17-24 : kuv | 200-350 | <10 | <30 | Tsheb roj thiab Lubrication systems | Roj kuj, Exllent ua, Zoo compression teeb |
| HNBR-P7043 | Peroxide | 43 | 50 ~ 100 | 70 | 17-24 : kuv | 200-350 | <10 | <30 | Cav gaskets, O-rings, Seals, Siv |
Roj kuj, Zoo compression teeb, Exllent ua |
| HNBR-P8043 | Peroxide | 43 | 50 ~ 100 | 80 | 17-24 : kuv | 200-350 | <10 | <30 | Drilling kav, Siab accumulators |
Roj kuj, Siab siab tsis kam, siab tempreture kuj |
1. Daim duab peb sab siv
2. Vibration Isolators
3.
Cov ntsaws ruaj ruaj
4. Thaum tshav kub kub resistant yeeb nkab
5.
Drilling tiv thaiv lub thawv
6. Pistons rau cov av nkos
7.
Sealing gaskets rau kev lag luam automotive
8. Cov ntsaws ruaj ruaj rau cov chaw nres tsheb fais fab
9.
Hydraulic hoses
10. Hydraulic foob
11. Cable sheaths rau cov chaw nres tsheb fais fab
12. Printing thiab ntaub chais
13. Cov ntsaws ruaj ruaj rau aerospace
14. Npog
15. Roj zais zis