Khoom:
Qhov kub tsis kam (-20 ° C txog + 250 ° C).
Exceptional tsis kam mus rau roj, fuels, hnyav, acids, thiab bases.
Lub zog tensile siab (10-20 MPa), qis compression teeb (<15% ntawm 150 ° C / 70h).
nplaim retardant (UL94 V-0 ntsuam xyuas) thiab ozone-resistant.
Qhov zoo:
Ua ntej sib xyaw nrog curatives (piv txwv li, bisphenol AF, peroxide) kom ua tau zoo vulcanization.
Retains dimensional stability nyob rau hauv aggressive chemical ib puag ncig.
FDA-raws li qib muaj rau zaub mov / kev kho mob.
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Aerospace: Roj system O-rings, cav ntsaws ruaj ruaj, thiab diaphragms.
Automotive: Turbocharger gaskets, kis cov ntsaws ruaj ruaj, thiab roj injectors.
Tshuaj: cov twj tso kua mis, lub rooj zaum valve, thiab hose sib dhos.
Khoom:
Thaum tshav kub kub tsis kam mus txog +150 ° C (nruab nrab +175 ° C).
Superior tsis kam rau roj, amines, thiab hydraulic kua.
Lub zog tensile siab (15-35 MPa) thiab qaug zog ua haujlwm.
Tsawg permeability rau gases.
Qhov zoo:
Pre-vulcanized rau txo cov sijhawm ua haujlwm.
Khaws elasticity nyob rau hauv lub sij hawm raug rau hnyav xov xwm.
Muaj nyob rau hauv peroxide- lossis sulfur-kho qib.
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Roj & Roj: Drilling packers, av nkos twj tso kua mis, thiab cov khoom siv lub taub hau.
Automotive: Siv sij hawm siv, roj txhaj tshuab, thiab turbocharger hoses.
Kev lag luam: Hydraulic lub tog raj kheej ntsaws ruaj ruaj thiab cov khoom siv gearbox.
Khoom:
Cov roj tsis zoo (zoo dua EPDM, tsawg dua HNBR).
Qhov kub thiab txias: -40 ° C txog + 120 ° C.
High abrasion tsis kam (ASTM D5963: 100-200 mm³ poob).
Zoo resilience thiab compression teeb kuj.
Qhov zoo:
Nqi-zoo nrog zoo moldability.
Customizable acrylonitrile cov ntsiab lus (18-50%) rau tailored roj kuj.
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Automotive: Roj hoses, O-rings, thiab kis cov ntsaws ruaj ruaj.
Industrial: Conveyor siv, luam ntawv rollers, thiab hydraulic seals.
Consumer: Latex hnab looj tes thiab cov khoom ua si.
Khoom:
Zoo tshaj ozone / huab cua tsis kam (5,000+ teev hauv QUV kuaj).
Qhov kub thiab txias: -50 ° C txog + 150 ° C.
High dielectric zog (20-30 kV / mm) thiab dej impermeability.
Tsawg roj permeability.
Qhov zoo:
Pre-formulated nrog antioxidants thiab UV stabilizers.
Kev co zoo heev damping (poob yam: 0.1-0.3).
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Automotive: Qhov rooj ntsaws ruaj ruaj, radiator hoses, thiab cav mounts.
Kev tsim kho: ru tsev membranes, pas dej liners, thiab qhov rais gaskets.
Hluav taws xob: Cable rwb thaiv tsev thiab fais fab kis txoj siv sia.
Khoom:
Lub zog tensile siab (20-60 MPa) thiab elasticity (txog 800% elongation).
Exceptional abrasion kuj (ASTM D5963: 20-50 mm³ poob).
Qhov kub thiab txias: -40 ° C txog + 100 ° C (txog + 120 ° C nrog cov cua sov stabilizers).
Resistant rau cov kuab tshuaj thiab hydrolysis.
Qhov zoo:
Customizable hardness (Shore A 50-95).
Muaj nyob rau hauv cam khwb cia, millable, los yog thermoplastic qib.
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Industrial: Log, rollers, thiab conveyor siv.
Automotive: Ncua bushings, shock absorbers, thiab CV sib koom khau boots.
Kev Kho Mob: Catheters, orthopedic braces, thiab prosthetics.
Khoom:
Kev kub ceev tsis tu ncua mus txog +150 ° C (nruam +175 ° C).
Kev tiv thaiv zoo heev rau cov dej tsis siv neeg kis tau tus mob (ATF), roj, thiab cua sov.
Nruab nrab ozone thiab huab cua tsis kam.
Tensile zog: 7-15 MPa.
Qhov zoo:
Ua ntej sib xyaw nrog amine lossis peroxide curatives rau kev kho sai.
Ua kom muaj kev ruaj ntseg nyob hauv ATF ib puag ncig.
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Automotive: Cov ntsaws ruaj ruaj, O-rings, thiab twj tso kua mis di
Fais fab steering system Cheebtsam.
Industrial: Pump seals rau roj-raws li xov xwm.
Khoom:
Dav kub ntau (-40 ° C rau + 150 ° C).
Ua rau cov roj, glycols, thiab huab cua.
Lub zog tensile siab (10-20 MPa) thiab compression teeb tsis kam.
Tsawg permeability rau gases.
Qhov zoo:
Balances tshav kub tsis kam thiab yooj.
Resistant rau hydrolysis thiab kev laus.
Muaj nyob rau hauv peroxide- lossis sulfur-kho qib.
Daim ca644f43fd429=Raws li tus neeg sawv cev txhawb nqa feem ntau siv hauv cov khoom siv roj hmab xim, silica tau ua lub luag haujlwm tseem ceeb.
Automotive: Radiator hoses, coolant system Cheebtsam, thiab cua nkag hoses.
Industrial: Conveyor siv rau tshuaj tuav thiab twj tso kua mis diaphragms.
HVAC: Cov kav dej sib txuas thiab kev vibration cais tawm.