Te Whakawhanaketanga o te Ethylene Propylene Diene Monomer (EPDM) Tino Elastic mo te Aatete Te Kohu Wai Maama Nui

Tirohanga: 0     Kaituhi: Kaiwhakatika Pae Wā Whakaputa: 2023-08-27 Takenga: Pae

Uiui

1 Te kowhiringa o te rapa mata

Pereti wera exchanger rapa gasket i te wa ano i te taha hau o te pāmahana teitei, taha wai o te mahi o te pēhanga tiketike, me te hoki i te whakapā ki te rangi, te tikanga mahi he ake tono. Na reira, kia tino pai te rauemi ki te whakakoi i te wera, a ka taea te tu ki te reo o te wai me tona mamaoa. I roto i nga ahuatanga penei, me whiriwhiri te hautanga papatipu propylene o te 40% ~ 50 % o te EPDM, na te mea ko tenei momo elasticity EPDM te pai rawa atu.

 

Ko te EPDM me te hautanga papatipu teitei o te toru o nga monomer he pai te elasticity me te iti o te huinga pupuhi; heoi, na te nui o te hononga-whakawhitinga, ka iti ake te kaha me te whakaroa i te wehenga, a, he ngoikore hoki te aukati o te koroheketanga. I tua atu, ko te kaha o te pakeke o te EPDM me te ENB i te mea ko te monomer tuatoru he pai ake i tera o te EPDM me te HD.

 

2 Pūnaha whakaora

Ko te tikanga, ka taea te whakangao i te rapa EPDM me nga momo punaha whakangao: peroxide me te whanariki kowhai kowhai. Ko te hanganga here-whakawhitinga o te punaha whakangao peroxide ko te here CC, ko te hononga hononga-whakawhitinga o te punaha whakangao whanariki he here CS. Ko te herenga CC he nui ake te waiariki i te herenga CS, na reira ka whakaraeraehia te rapa EPDM whakawera teitei ki te peroxide. Ko te peroxide tino whakamahia ko DCP. Na te pikinga o te inenga DCP, ka huri haere te rapa puia mai i te undersulfurization tuatahi, te iti o te kaha me te rerekee nui ki te piki o te kaha me te heke o te deformation; katahi ka piki ake te tohu o te vulcanization, ka tiimata te heke o te kaha, ka tae ki te iti rawa te rereketanga; I te mutunga, i muri i te nui o te kaikawe vulcanizing, ka timata te wahanga o te mekameka ngota ki te pakaru i te heke o te mekameka, ka heke haere tonu te kaha, ka piki haere te rereketanga.

 

3.Whakakii

Ko te EPDM no te rapa kore-kiriata, karekau te kaha o te rapa mata i te teitei. Engari i muri i te taapiri i te whakakii whakakii, ka nui haere te kaha. Ko te whakakaha i te whakakii i te nuinga o te waa he iti te paanga ki te aukati wera, engari ko te whakanui ake i te nui o te whakakii ka awhina tonu ki te whakapai ake i te aukati wera o te rapa, engari ka whakaitihia nga utu.

 

Ka piki ake te karaehe o te waro pango, ka heke te huinga kōpeketanga, ka piki te elasticity, ka heke te kaha. Ko te kaha o te N990 waro pango he iti rawa, he uaua ki te whakahaere i roto i te hanga, na reira kaore e whakamahia. Mā te kōwhiri i te N762 waro pango, ka taea te whiwhi i te uara huinga kōpeke iti. Hei whakahaere i te whakamararatanga o te waro pango me te pai o te mahi tukatuka, whiriwhiria he hinu paraffini iti, he tino hototahi ki te rapa ethylene propylene.

 

4. Kaitohu whakawhiti

Karekau he herenga haunga i runga i te mekameka matua o te EPDM, ahakoa ka taea te whakamahi i te peroxide vulcanization, engari he puhoi te tere vulcanization, he iti te pai o te whakawhiti. Hei whakapumau me te whakatere i te tukanga vulcanization, he mea tika ki te whakamahi i te kaihoko whakawhiti. He pai ake te TAC/GR mo te whakamararatanga me te pauna.

 

Na te pikinga o te nui o te TAC/GR, ka heke te kaha o te kaha, te elongation i te wehenga me te whakakoi i te whakarereketanga pumau o te rapa puia, ka piki ake te uara MH o te ahotea tensile tonu. Ka kitea i pai ake te kiato whakawhiti o te rapa puia, kua heke nga ahuatanga miihini, engari kua nui ake te elasticity. I te wa ano, ka heke te uara o te ML, e tohu ana kua heke iho te viscosity Mooney  , kua piki ake te wai o te rapa, a he ngawari ki te tukatuka; Ko te ts1 kaore i rereke, ka whakapotohia te uara t 90, ka tino pai ake te tere o te whakangao. He iti ake te mahi tawhito i te 1.5phr o TAC/GR. Ko tenei pea na te mea he awhina whakawhiti-hono, whakahohe i te tukanga whakangao peroxide, whakapoto i te wa whakangao, whakaitihia te tupono o te pakaru o te mekameka rapa me te koretake i te teitei o te wera. Ina he nui rawa te moni, ka whakanuia e ia te tawhito-whakawhitiwhiti o te rapa me te whakaiti i te parenga wera o te EPDM. Whai muri i te whakatairite, he pai ake te 2phr i te 2phr, a kaore i te tino patunga tapu te parenga wera, no reira ka whakamahia te TAC/GR i te 2phr.

 

5.Tauora

Ka taea te whakamahi i te EPDM mo te wa roa i te 150 , engari i tua atu i te 150 , ka timata te tau o te ngota ngota, a i te 180 , ka ata pirau te mekameka ngota rapa. Hei whakapai ake i tana mahi i nga wera nui, me whakamahi nga taapiri whakamarumaru. I roto i te take o te paoho wai-kohu, ka taea te whakamahi i te antioxidant RD, he atete ki nga wera teitei engari kaore e pa ki te whakangao. I tua atu, ka taea te whakamahi 0.5phr antioxidant D ki te whakapakari i te kaha ki te aukati i te hāora i roto i te hau me te whakapai ake i te aukati ngenge. Ko te ōwehenga o RD/anti-butyl=1.8/0.5.

 

Whakamutunga

Ko te whakawhanaketanga o te rapa teitei elasticity EPDM te kohu wai-nui, ko te arotahi ko te whakatutuki i nga taonga miihini i raro i te kaupapa o te whakanui ake i te aukati tawhito me te whakaiti i te uara huringa pumau.

(1) Ko te rapa EPDM raw kua tohua me te 40% ~ 50% o te propylene me te hautanga papatipu reo o te ENB hei monomer tuatoru.

( 2) Ka whakamahia e te punaha vulcanization te DCP / TAC, e awhina ana ki te whakapai ake i te pai o te honohono, te atete tawhito me te mahi tukanga.

( 3) Whakamahia te N762 waro pango elasticity teitei ka taea, ka taea te whakapai ake i te aukati ki te uruhanga pāpāho me te mahi tawhito, ka taea te whakaiti i te utu.

( 4) Whakapaia te punaha whakamarumaru o te antioxidant RD/antioxidant D, me te antioxidant RD te pāmahana teitei hei mea matua, me te antioxidant D hei awhina mo te ngenge me te ozone-aukati.

( 5) Ko te tukanga whakaputa e tango ana i te vulcanization tuarua teitei-te pāmahana ki te whakanui ake i te tohu o te vulcanization.

(6) Ko te mahi a te EPDM i roto i te wai wera me te kohu wai he pai ake i tera i te hau (he rite tonu te pāmahana). Engari ahakoa, ko tana whakamahinga mo te wa roa o te pāmahana kaore e neke ake i te 150 ; Ko te paanga o te paanga o te 165 e tika ana, ko te teitei e kore e neke ake i te 180 .


NGA LINKO Tere

O TATOU HUA

HE KORERO WHAKAPAKI

Tāpirihia: No.33, Lane 159, Taiye Road, Takiwa Fengxian, Shanghai
Waea / WhatsApp / Skype: +86 15221953351
Ī-mēra:  info@herchyrubber.com
Mana pupuri     2023 Shanghai Herchy Rubber Co., Ltd. Mahere pae |   Kaupapahere Tūmataiti | Tautoko Na Leadong.