GA-10×3
Hercy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x 5min x 15MPa
| Product parameters | |||||||
| Product | GA-1023 | GA-1033 | GA-1043 | GA-1053 | GA-1063 | GA-1073 | GA-1083 |
| Appearance | Translucent | ||||||
| Williamplasticity | 100 | 115 | 150 | 205 | 240 | 280 | 310 |
| Hardness (ShoreA) | 20 | 30 | 40 | 50 | 60 | 70 | 80 |
| Density(g/cm3) | 1.08 | 1.10 | 1.12 | 1.16 | 1.19 | 1.22 | 1.22 |
| Tensilestrength (MPa) | 6 | 7 | 8 | 9 | 8 | 8 | 7 |
| Elongation(%) | 900 | 750 | 650 | 550 | 450 | 350 | 150 |
| Tearstrength (kN/m) | 10 | 16 | 20 | 20 | 20 | 20 | 16 |
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175° x 5min x 15MPa
| Product parameters | |||||||
| Product | GA-1023 | GA-1033 | GA-1043 | GA-1053 | GA-1063 | GA-1073 | GA-1083 |
| Appearance | Translucent | ||||||
| Williamplasticity | 100 | 115 | 150 | 205 | 240 | 280 | 310 |
| Hardness (ShoreA) | 20 | 30 | 40 | 50 | 60 | 70 | 80 |
| Density(g/cm3) | 1.08 | 1.10 | 1.12 | 1.16 | 1.19 | 1.22 | 1.22 |
| Tensilestrength (MPa) | 6 | 7 | 8 | 9 | 8 | 8 | 7 |
| Elongation(%) | 900 | 750 | 650 | 550 | 450 | 350 | 150 |
| Tearstrength (kN/m) | 10 | 16 | 20 | 20 | 20 | 20 | 16 |