Test: AB ratio of 1 :1, 130°C x 5min x 15MPa
| Product parameters |
|
| Product | GA-2040D
| GA-2040D-45
| GA-20400-60
|
| Appearance | Light grey/camel/red | Light grey | Grey |
ViscosityA (Pa·s)
| 250-400 | 70-100 | 1500-2000
|
ViscosityB (Pa·s)
| 250-400 | 70-100 | 1500-2000 |
| Hardness (ShoreA) | 43-48 | 37-43 | 55-60 |
| Density(g/cm3) | 1.11
| 1.11
| 1.15
|
| Tensile strength (MPa) | 7
| 7.0
| 8.5
|
| Elongation(%) | 500 | 450 | 550 |
| Tear strength (kN/m) | 22
| 22
| 35
|
| Dielectric constant at 100HZ | 3.03 | 2.95
| 3.3 |
| Dissipation factor at100HZ | 0.0016 | 0.0017 | 0.004 |
| Resistance to electric leakage and marking | 1A3.5 | 1A4.5 | 1A3.5 |
| DielectricStrength (kV/mm) | 24 .3
| 20.5
| 22
|
| VolumeResistivity (Ω·cm) | 1.0 *1015 | 1.0 *1015 | 1.0 *1015 |
| Flame class | FV-0 | FV-0 | FV-0 |