GA-10 × 3 Silicone kapiira fr okubumba n'amaanyi amangi (HCR)

Okukozesa: ebintu eby'enjawulo, ebikozesebwa mu ffumbiro, ebikozesebwa mu kuwuga n'ebintu ebiralawith complex structure.oKey features: okuwonya amangu, amaanyi amangi, processab川ty ennungi ennyo,pass theauthentication of RoHS, REACH, ne FDA.
  • GA-10×3

  • Hercy

Ebiriwo:
Omuwendo:

Okugezesa: 1% eky’ekirungo ekiwonya (50% ekikuta kya DBPMH mu silicone gum), 175° x 5min x 15MPa


Ebipimo by’ebintu ebikolebwa
Ekyamaguzi GA-1023
GA-1033 GA-1043 GA-1053 GA-1063 GA-1073 GA-1083
Endabika Etangalijja
Obuveera bwa William
100
115
150
205
240
280
310
Obukaluba (ShoreA) .
20
30
40
50
60
70
80
Obugumu(g/cm3) . 1.08
1.10
1.12
1.16
1.19
1.22
1.22
Obugumu bw’okusika (MPa) .

6
7
8
9
8
8
7
Okuwanvuwa(%) . 900
750
650
550
450
350
150
Obugumu bw’amaziga (kN/m) . 10
16
20
20
20
20
16





Jjuuzi: 
Ekiddako: 

ENKOZESA Y'AMAWANGA

EBINTU EBYAFFE

AMAWULIRE AG'OKUKWATAGANA

Gattako: No.33, Lane 159, oluguudo lwa Taiye, mu Disitulikiti y’e Fengxian, Shanghai
Essimu / WhatsApp / Skype ku ssimu: +86 15221953351
Eddembe ly’okuwandiika     2023 Kkampuni ya Shanghai Herchy Rubber Co., Ltd. Sitemap y'ekifo |   Enkola y'Ebyama | Obuwagizi Bwa... Leadong.