GA-96XX
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Application: suitable for the production of heat conductive silicone rubber tape, thermal conductive gasket and so on.
Key features: high strength, thermal conductivity can reach 0.5 -2w/m x k, pass theauthentication of RoHS and REACH.
Test: 1% of curing agent (50% paste of DBPMH in siliconegum), 175℃x5min x 15MPa.
| Product parameters | ||||||||
| Product | GA-9630 | GA-9640 | GA-9650 | GA-9660 | GA-9670 | GA-9680 | GA-9680B | |
| Appearance | Gray | Black | ||||||
| William plasticity | 160 | 180 | 200 | 220 | 240 | 270 | 270 | |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | 70 | 76 | 79 | |
| Density(g/cm3) | 2.1 | 2.13 | 2.15 | 2.2 | 2.25 | 2.04 | 2.35 | |
| Tensile strength (MPa) | 1 | 1.5 | 2 | 2 | 2.5 | 4.5 | 4.7 | |
| Elongation(%) | 800 | 750 | 700 | 600 | 500 | 80 | 130 | |
| Tear strength (kN/m) | 6 | 6 | 6 | 10 | 10 | 8 | 11.3 | |
| Coefficient of thermal conductivity(W/MK) | 0.8 | 0.8 | 0.8 | 0.9 | 0.9 | 0.8 | 0.9 | |