GA-2430
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A/B ratio is adjustable, 130°Cx 5min x 15MPa.
| Product parameters | ||||
| Product | GA-2430 | GA-2440 | GA-2450 | |
| Appearance | Translucent | |||
| A/B配比A/Bratio | 2:100 |
2:100 |
2:100 |
|
| B剂粘度Viscosity of part-B (Pa·s) |
10-200 | 10-200 | 10-200 | |
| Hardness (ShoreA) | 28 | 38 |
50 |
|
| Density(g/cm3) | 1.08 |
1.06 | 1.10 | |
| Tensile strength (MPa) | 4.0 |
4.5 |
7.0 |
|
| Elongation(%) | 300 | 250 | 350 | |
| Tear strength (kN/m) | 10 | 15 | 15 | |
| Linearshrinkage(%) | 2.1 | 2.1 |
2.0 |
|