GA-2100D
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A:B ratio of 1:1, 130℃ x 5min x 15MPa.
| Product parameters | |||||||
| Product | GA-2100D | GA-2105D | GA-2110D | GA-2115D | GA-2120D | GA-2125D | |
| Appearance | Translucent | ||||||
| Viscosity(Pa.s) |
A:1.0 B:1.0 |
A:4.0 B:4.0 |
A:3.0 B:3.0 |
A:3.5 B:3.5 |
A:4.6 B:4.3 |
A:4.5 B:4.5 |
|
| Hardness (ShoreA) | 0 | 5 | 10 | 15 |
20 |
25 |
|
| Density(g/cm3) | 1.10 |
1.10 |
1.12 |
1.12 | 1.10 |
1.12 |
|
| Tensile strength (MPa) | 0.4 |
2.5 |
3.0 |
4.0 |
6.0 |
6.0 |
|
| Elongation(%) | 500 | 500 | 600 | 550 | 600 |
600 |
|
| Tear strength (kN/m) | 1.5 | 8 | 7 |
8 | 11 |
14 |
|