GA-10 × 3 Silicone rɔba fr nwene a ahoɔden a ɛkorɔn (HCR) .

Dwumadi: nneɛma ahorow, kitchenware, asuguare nneɛma ne nneɛma afoforo a ɛyɛ den structure.oKey features: ntɛmntɛm curing, ahoɔden a ɛkorɔn, excellent processab川ty,pass theauthentication of RoHS, REACH, ne FDA.
  • GA-10 × 3 na ɛwɔ hɔ

  • Hercy na ɔkyerɛwee

Nea Ɛwɔ Hɔ:
Dodow:

Sɔhwɛ: 1% a ɛyɛ aduru a wɔde sa yare (50% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175° x 5min x 15MPa


Product parameters .
Adwadeɛ GA-1023 na ɛwɔ hɔ
GA-1033 na ɛwɔ hɔ GA-1043 na ɛwɔ hɔ GA-1053 na ɛwɔ hɔ GA-1063 na ɛwɔ hɔ GA-1073 na ɛwɔ hɔ GA-1083 na ɛwɔ hɔ
Mmaeɛ Translucent .
Williamplasticity a wɔde yɛ nneɛma
100
115
150
205
240
280
310
Hardness (Shorea) .
20
30
40
50
60
70
80
density(g/cm3) . 1.08
1.10
1.12
1.16
1.19
1.22
1.22
Ahoɔden a ɛtwetwe ade (MPa) .

6
7
8
9
8
8
7
Elongation(%) . 900
750
650
550
450
350
150
Nusu ahoɔden (kN/m) . 10
16
20
20
20
20
16





Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.