GA-10×3 Silicone roba fr gyare-gyare tare da babban ƙarfi (HCR)

Aikace-aikacen: abubuwa daban-daban, kayan dafa abinci, kayan ninkaya da sauran samfuran tare da hadadden tsari.oKey fasali: saurin warkewa, ƙarfi mai ƙarfi, kyakkyawan tsari mai ƙarfi, ƙaddamar da amincin RoHS, REACH, da FDA.
  • GA-10×3

  • Hercy

samuwa:
Yawan:

Gwaji: 1% na wakili mai warkarwa (50% manna DBPMH a cikin danko silicone), 175° x 5min x 15MPa


Siffofin samfur
Samfura GA-1023
GA-1033 GA-1043 GA-1053 GA-1063 GA-1073 GA-1083
Bayyanar Translucent
Williamplasticity
100
115
150
205
240
280
310
Hardness (ShoreA)
20
30
40
50
60
70
80
Girma (g/cm3) 1.08
1.10
1.12
1.16
1.19
1.22
1.22
Ƙarfin ƙarfi (MPa)

6
7
8
9
8
8
7
Tsawaita(%) 900
750
650
550
450
350
150
Ƙarfin hawaye (kN/m) 10
16
20
20
20
20
16





Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.