GA-10×3
Hercy
| Availability: | |
|---|---|
| Quantity: | |
Fitsapana: 1% amin'ny fanafody manasitrana (50% amin'ny DBPMH amin'ny silikôma silikônina), 175° x 5min x 15MPa
| Masontsivana vokatra | |||||||
| vokatra | GA-1023 |
GA-1033 | GA-1043 | GA-1053 | GA-1063 | GA-1073 | GA-1083 |
| Bika Aman 'endrika | Translucent | ||||||
| Williamplasticity |
100 |
115 |
150 |
205 |
240 |
280 |
310 |
| Hardness (ShoreA) |
20 |
30 |
40 |
50 |
60 |
70 |
80 |
| Hateza (g/cm3) | 1.08 |
1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| Henjana (MPa) |
6 |
7 |
8 |
9 |
8 |
8 |
7 |
| Elongation(%) | 900 |
750 |
650 |
550 |
450 |
350 |
150 |
| Hain-dranomaso (kN/m) | 10 |
16 |
20 |
20 |
20 |
20 |
16 |