GA-10×3 Silikon kawotchou pou bòdi ak gwo fòs (HCR)

Aplikasyon: atik divès, istansil kwizin, founiti pou naje ak lòt pwodwi ak estrikti konplèks. Karakteristik kle: geri rapid, gwo fòs, pwosesis ekselan, pase otantifikasyon RoHS, REACH, ak FDA.
  • GA-10×3

  • Hercy

Disponibilite:
Kantite:

Tès: 1% nan ajan geri (50% keratin nan DBPMH nan jansiv silikon), 175 ° x 5min x 15MPa


Paramèt pwodwi
Pwodwi GA-1023
GA-1033 GA-1043 GA-1053 GA-1063 GA-1073 GA-1083
Aparans Translusid
Williamplasticity
100
115
150
205
240
280
310
Dite (ShoreA)
20
30
40
50
60
70
80
Dansite (g/cm3) 1.08
1.10
1.12
1.16
1.19
1.22
1.22
Fòs traction (MPa)

6
7
8
9
8
8
7
elongasyon (%) 900
750
650
550
450
350
150
Fòs chire (kN/m) 10
16
20
20
20
20
16





Previous: 
Pwochen: 

Lyen RAPID

PWODWI NOU YO

ENFÒMASYON KONTAK

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Dwa     2023 Shanghai Herchy Rubber co, Ltd. Sitemap |   Règleman sou enfòmasyon prive | Sipòte By Leadong.