GA-2039M
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa
| Product parameters | |||||
| Product | GA-2039M | GA-2049M | GA-2059M | GA-2069M | |
| Appearance | Translucent | ||||
| Viscosity(Pa.s) | A:1000 B:2000 | A:1000 B:2000 | A:1000 B:2000 | A:1000 B:2000 | |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | |
| Density(g/cm3) | 1.13 | 1.12 | 1.12 | 1.14 | |
| Tensile strength (MPa) | 6 | 6 | 6 | 5 | |
| Elongation(%) | 600 | 550 | 450 | 350 | |
| Tear strength (kN/m) | 10 | 10 | 15 | 20 | |