Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa
| Product parameters | ||||||
| Product | GA-2031W | GA-2041W | GA-2051W | GA-2061W | GA-2071W | |
| (A/B)Appearance | (While/Black) | (While/Black) | (While/Black) | (While/Black) | (While/Black) | |
| Hardness (ShoreA) | 32 | 43 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.3 | 1.3 | 1.36 | 1.36 | 1.52 | |
| Tensile strength (MPa) | 4.5 | 4.5 | 5.0 | 4.5 | 4.0 | |
| Elongation(%) | 300 | 300 | 300 | 200 | 140 | |
| Tear strength (kN/m) | 10 | 10 | 12 | 12 | 8.0 | |