GA-10 × 3 caag Silikoon fr qaabaynta leh xoog sare (HCR)

Codsiga: alaabo kala duwan, qalabka jikada, agabka dabaasha iyo alaabada kale ee leh qaab dhismeed adag
  • GA-10×3

  • Hercy

Helitaanka:
Tirada:

Tijaabada: 1% ee wakiilka daawaynta (50% koollada DBPMH ee xanjada silikoonka), 175° x 5min x 15MPa


Xuduudaha alaabta
Alaabta GA-1023
GA-1033 GA-1043 GA-1053 GA-1063 GA-1073 GA-1083
Muuqashada Translucent
Williamplasticity
100
115
150
205
240
280
310
Adag ( ShoreA)
20
30
40
50
60
70
80
Cufnaanta (g/cm3) 1.08
1.10
1.12
1.16
1.19
1.22
1.22
Xoog adkaysi (MPa)

6
7
8
9
8
8
7
Dheeraynta(%) 900
750
650
550
450
350
150
Xoogga ilmada (kN/m) 10
16
20
20
20
20
16





Kii hore: 
Xiga: 

XIDHIIDHYADA DEGDEGGA AH

Alaabooyinkayaga

MACLUUMAADKA XIRIIRKA

Kudar: No.33, Lane 159, Wadada Taiye, Degmada Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Xuquuqda daabacaadda     2023 Shanghai Herchy Rubber Co., Ltd. Khariidadda goobta |   Siyaasadda Qarsoonnimada | Taageerada By Leadong.