GA-2525
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa
| Product parameters | |||||||
| Product | GA-2525 | GA-2530 | GA-2540 | GA-2850 | GA-2860 | GA-2870 | |
| Appearance | Translucent | ||||||
| Viscosity(Pa.s) | 80 | 80 | 80 | 220 | 300 | 400 | |
| Hardness (ShoreA) | 25 | 30 | 40 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.08 | 1.10 | 1.11 | 1.13 | 1.14 | 1.16 | |
| Tensile strength (MPa) | 4.5 | 5.0 | 5.5 | 6.0 | 6.0 | 5.0 | |
| Elongation(%) | 400 | 350 | 300 | 250 | 220 | 180 | |
| Tear strength (kN/m) | 12 | 14 | 18 | 20 | 18 | 16 | |
| Linearshrinkage(%) | 2.0 | 2.0 | 2.0 | 2.0 | 2.0 | 2.0 | |