Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa
| Product parameters | |||||||
| Product | GA-2820 | GA-2830 | GA-2840 | GA-2850 | GA-2860 | GA-2870 | |
| Appearance | Translucent | ||||||
| Viscosity(Pa.s) | 2000 | 2500 | 3000 | 3500 | 4000 | 4000 | |
| Hardness (ShoreA) | 20 | 30 | 40 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.10 | 1.10 | 1.11 | 1.12 | 1.13 | 1.14 | |
| Tensile strength (MPa) | 6.5 | 7.5 | 9.0 | 9.5 | 9.5 | 9.0 | |
| Elongation(%) | 850 | 780 | 650 | 500 | 400 | 300 | |
| Tear strength (kN/m) | 12 | 15 | 30 | 35 | 30 | 30 | |
| Linearshrinkage(%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 | 2.0 | |