Ethylene Propylene Rubber – EPDM/EPM
The main performance advantages of EPDM are as follows.
(1) High cost performance, with a raw rubber density of only 0.86-0.90g/cm3, which is the lightest common rubber with raw rubber density; and it can be bottled in large quantities to reduce rubber costs.
(2) Excellent aging resistance, weather resistance, ozone resistance, sunlight resistance, heat resistance, water resistance, water vapor resistance, UV resistance, radiation resistance and other aging properties. When EPDM is used in combination with other unsaturated diene rubbers such as NR, SBR, BR, NBR, CR, etc., it can act as a polymer antioxidant or anti-aging agent.
(3) Excellent chemical resistance, acid, alkali, detergent, animal and vegetable oils, alcohol, ketone, etc.; excellent water resistance, superheated water, water vapor resistance; polar oil resistance.
(4) Excellent insulation performance, volume resistivity 1016Ω-cm, breakdown voltage 30-40MV/m, dielectric constant (1kHz, 20℃) 2.27.
(5) Wide operating temperature range, minimum operating temperature -40-60℃, can be used for a long time below 130℃.
Hirsch Rubber exports EPDM/EPM to 15 countries including the United States, Russia, Brazil, Argentina, South Korea, Germany, Italy, Spain, Australia, and India.
Ethylene Propylene Rubber-EPDM/EPM
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ethylene Content | ENB Content | Extend-oil Content | Application | Character |
| Grade | ML(1+4)100℃ | ML(1+4)125℃ | ML(1+4)150℃ | wt% | wt% | PHR | ||
| S501A | 44 | [30] | 53 | 4.1 | Injection Molding Products ;High hardness products; | Low Mooney viscosity; Good liquidity; Low temperature resistance; | ||
| S505A | 45 | [29] | 55 | 9.4 | High hardness products;Tire sidewall;Foamed parts; | Low Mooney viscosity; Good liquidity; High ENB content; Fast curing speed; Low temperature resistance; | ||
| S537-3 | 35 | 57 | 2.3 | Inner tube;Shoe;Construction machinery parts | High temperature resistance; Low temperature resistance; | |||
| S537-2 | 40 | 57 | 3 | Inner tube;Construction machinery parts | High temperature resistance; Low temperature resistance; | |||
| S512F | 63 | 69 | 4.5 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | |||
| S5890F | [87] | 64 | 68 | 5.5 | Hose;Dense sealing strip;Gasket; | High filling; Excellent processing property; | ||
| S552 | 84 | 58 | 4.1 | Hose;Dense sealing strip;Gasket;Industrial products; | Excellent processing property; Low temperature resistance; High mechanical properties | |||
| S552-1 | 84 | 58 | 5.7 | Hose;Dense sealing strip;Industrial products; | Excellent processing property; Low temperature resistance; High mechanical properties; High rebound | |||
| S553 | [98] | 72 | 62 | 4.5 | Door and window sealing strips;Waterproof; | High Mooney viscosity; High filling; Low temperature resistance; High mechanical properties; | ||
| S5206F | [84] | 81 | 60 | 8.5 | Sponge profile;Foamed parts; | High Mooney viscosity; High ENB content; Fast curing speed; High mechanical properties; | ||
| S5527F | [109] | 81 | 60 | 8.5 | Sponge profile;Foamed parts;High rebound products; | High filling; High Mooney viscosity; High ENB content; Fast curing speed; High mechanical properties; | ||
| S6090WF | 53 | 70 | 5.7 | 50 | Low hardness products;Hose;Washing machine door seals;Automobile wire harness;High rebound products;High mechanical properties | High ethylene content; High Mooney viscosity; High mechanical properties; Excellent processing property; | ||
| S600WF | 61 | [41] | 72 | 4 | 100 | Low hardness products;Bicycle tyre;Automobile wire harness;High rebound products;High mechanical properties | High filling; High mechanical properties; Excellent processing property; | |
| S7486F | 92 | 67 | 60 | 9 | Sponge profile;Dense sealing strip;Foamed parts; | Low ethylene content; High ENB content; Fast curing speed; | ||
| S6075WF | 50 | 60 | 4.7 | 75 | Low hardness products;Injection Molding Products ;Automobile wire harness;High mechanical properties | Low ethylene content; High Mooney viscosity; Excellent processing property; Low temperature resistance; |
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ethylene Content | ENB Content | Extend-oil Content | Application | Character |
| Grade | ML(1+4)100℃ | ML(1+4)125℃ | ML(1+4)150℃ | wt% | wt% | PHR | ||
| J-2070 | 44* | 57.8 | 1.9 | Inner tube;Shoe;Construction machinery parts | High temperature resistance;Low temperature resistance; | |||
| J-2080 | 53 | 62 | 2 | Inner tube;Shoe;Construction machinery parts | High temperature resistance;Low temperature resistance;High mechanical properties | |||
| 3062E | 41 | 68.5 | 3.9 | 20 | Injection Molding Products ;Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | ||
| J-3060P | 45 | 68.5 | 4 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | |||
| J-3080 | 70 | 68.5 | 4 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | |||
| J-3080P | 70 | 68.5 | 4 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | |||
| J-3092E | 60 | 57.2 | 4.6 | 20 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | ||
| 4045 | 45 | 52 | 7.7 | High hardness products;Tire sidewall;Foamed parts; | Low Mooney viscosity; Good liquidity; High ENB content; Fast curing speed; Low temperature resistance; | |||
| J-4090 | 65 | 52.5 | 7.7 | Tire sidewall;Foamed parts; | High ENB content; Fast curing speed; Low temperature resistance; |
| Herchy | Mooney viscosity | Mooney viscosity | Mooney viscosity | Ethylene Content | Propylene Content | ENB Content | Extend-oil Content | Application | Character |
| Grade | ML(1+4)100℃ | ML(1+4)125℃ | ML(1+4)150℃ | wt% | wt% | wt% | PHR | ||
| CO 033 | 30 | 72 | 28 | ||||||
| CO 034 | 44 | 72 | 28 | ||||||
| CO 038 | 60 | 72 | 28 | ||||||
| CO 043 | 33 | 55 | 45 | ||||||
| CO 054 | 44 | 59 | 41 | ||||||
| CO 058 | 80 | 60 | 52 | 48 | |||||
| CO 059 | 79 | 59 | 41 | ||||||
| TER 4033 | 30 | 70 | 25 | 5 | High hardness products;Injection Molding Products;Automobile rubber seal strip | Low Mooney viscosity; Good liquidity; High ethylene content; High mechanical properties; Excellent processing property | |||
| TER 4038EP | 60 | 68.6 | 27 | 4.4 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | |||
| TER 4039 | 77 | 68.6 | 27 | 4.4 | Hose;Door and window sealing strips;Extrusion Product; | High ethylene content; High mechanical properties; Excellent processing property | |||
| TER 4044 | 44 | 61 | 35 | 4 | Injection Molding Products ;High hardness products; | Low Mooney viscosity; Good liquidity; High mechanical properties; Excellent processing property | |||
| TER 4047 | 55 | 55.5 | 40 | 4.5 | Brake Hose;Molded products ;Gasket;Construction machinery parts;Inner tube;Shoe; | Low ethylene content; Excellent processing property; Low temperature resistance | |||
| TER 4049 | 76 | 55.5 | 40 | 4.5 | Hose;Dense sealing strip;Gasket;Industrial products; | Low ethylene content; High mechanical properties; Low temperature resistance | |||
| TER 4334 | 28 | 68.3 | 27 | 4.7 | 43 | High hardness products;Injection Molding Products;Automobile rubber seal strip;Industrial products | Low Mooney viscosity; Good liquidity; High ethylene content; High mechanical properties; Excellent processing property | ||
| TER 4436 | 43 | 66.5 | 28 | 5.5 | 67 | Washing machine door seals;Industrial products | Excellent processing property; High mechanical properties; | ||
| TER 4437 | 57 | 63.5 | 32 | 4.5 | 67 | Washing machine door seals;Industrial products; | Excellent processing property; High mechanical properties; High temperature resistance; | ||
| TER 4535 | 32 | 64.6 | 32 | 3.4 | 100 | Washing machine door seals;Molded products ; | Low ENB content; High temperature resistance; | ||
| TER 6148 | 65 | 53 | 40 | 7 | 18 | Foamed parts;Sponge profile;Molded products ; | Low ethylene content; High ENB content; Fast curing speed; Low temperature resistance | ||
| TER 6235 | 33 | 60.6 | 32 | 7.4 | 30 | Inner tube;Shoe;Foamed parts;Sponge profile;Molded products | Low Mooney viscosity; Good liquidity; High ethylene content; High mechanical properties; Excellent processing property; High ENB content; Fast curing speed; | ||
| TER 6537 | 43 | 60 | 32 | 8 | 100 | Foamed parts;Sponge profile;Washing machine door seals;Molded products | High ENB content; Fast curing speed; | ||
| TER 9046 | 67 | 60.1 | 31 | 8.9 | Foamed parts;Sponge profile;Industrial products | High ENB content; Fast curing speed; | |||
| TER 4548 | 47 | 59.5 | 36 | 4.5 | 10 | Inner tube;Shoe;Molded products ;Industrial products;Molded products | Low Mooney viscosity; Good liquidity; | ||
| TER 8148 | 68 | 52.5 | 39 | 8.5 | 21 | Foamed parts;Sponge profile;Industrial products;Molded products | Low ethylene content; High ENB content; Fast curing speed; Low temperature resistance | ||
| TER 7040 | 87 | 53.5 | 40 | 6.5 | Hose;Door and window sealing strips;Extrusion Product; | Low ethylene content; High filling; High Mooney viscosity; High mechanical properties; Low temperature resistance | |||
| TER 4049 | 76 | 55.5 | 40 | 4.5 | Hose;Door and window sealing strips;Extrusion Product; | Low ethylene content; Low temperature resistance | |||
| TER 5029 | 80 | 69.5 | 25 | 5.5 | Hose;Door and window sealing strips;Extrusion Product; | High filling; High ethylene content; High Mooney viscosity; High mechanical properties |
1. Automotive sealing strip
Sealing strip for hood
Door seal
Window screen
Sunroof sealing
Truck seal
Anti-dust
Glassrun channel
Anti-noise
2. Hose
Brake hoses
Automotive radiator hose
Skylight drain pipe
3. Wire and cable
Power cable
Rubber sheathed cable
Local cable
Television cable
Instrument cable
4. Waterproof coil
Wall waterproof coil
Roof waterproof coil
Highway waterproof roll
Tunnel waterproof coil
5. Tires
Inner tube
Tire side
Bicycle tire
6. Ordinary molded products
Rubber block
Rubber mat
Gasket
Brake bowl
7. Oil modification and other fields
lubricant additive