Su'ega: 1% o le vaila'au fa'amalolo (50% fa'apipi'i o le DBPMH i le pulu silicone), 175° x 5min x 15MPa
| Fa'asologa o oloa | |||||||
| Oloa | GA-1023 |
GA-1033 | GA-1043 | GA-1053 | GA-1063 | GA-1073 | GA-1083 |
| Fa'aaliga | Translucent | ||||||
| Williamplasticity |
100 |
115 |
150 |
205 |
240 |
280 |
310 |
| Malosi (ShoreA) |
20 |
30 |
40 |
50 |
60 |
70 |
80 |
| Malosi (g/cm3) | 1.08 |
1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| Malosi (MPa) |
6 |
7 |
8 |
9 |
8 |
8 |
7 |
| Fa'atele(%) | 900 |
750 |
650 |
550 |
450 |
350 |
150 |
| Malosi loimata (kN/m) | 10 |
16 |
20 |
20 |
20 |
20 |
16 |