GA - 10 × 3.
Hercy
| Go hwetšagala: | |
|---|---|
| Palo: . | |
Teko: 1% ya moemedi wa go fodiša (50% ya peista ya DBPMH ka gare ga mare a silicone), 175 ° x 5min x 15MPa
| Ditekanyetšo tša Setšweletšwa . | |||||||
| Setšweletšwa | GA - 1 0 2 3 |
GA - 1 0 3 3 | GA - 1 0 4 3 | GA - 1 0 5 3 | GA-1063 ya go swana le | GA-1073 ya go swana le yona | GA-1083 ya go swana le |
| Ponagalo | Translucent . | ||||||
| Williamplasticity . |
100 |
115 |
150 |
205 |
240 |
280 |
310 |
| Go thatafala (Sorea) . |
20 |
30 |
40 |
50 |
60 |
70 |
80 |
| Kitlano (G / CM3) . | 1.08 |
1.10 |
1.12 |
1.16 |
1.19 |
1.22 |
1.22 |
| Matla a go goga (MPa) . |
6 |
7 |
8 |
9 |
8 |
8 |
7 |
| go telefa (%) . | 900 |
750 |
650 |
550 |
450 |
350 |
150 |
| Matla a megokgo (kN / m) . | 10 |
16 |
20 |
20 |
20 |
20 |
16 |