GA-2040
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 130°C x 10min, 200°C x 4H.
| Product parameters | |||||
| Product | GA-2040-35T | GA-2040-35 | GA-2050-35 | GA-2040-45 | |
| Appearance | Translucent | Grey | Red | Grey | |
| Hardness (ShoreA) | 35-42 | 35-42 | 48 | 42 | |
| Density(g/cm3) | 1.13 | 1.13 | 1.14 | 1.12 | |
| Tensile strength (MPa) | 9.5 | 9.5 | 9.0 | 9.5 | |
| Elongation(%) | 800 | 800 | 650 | 800 | |
| Tear strength (kN/m) | 40 | 40 | 35 | 40 | |
| Hot age resistance 153°C±3°C×7D | Change of tensile strength(%) | <土10 | <土10 | <土10 | <土10 |
| Change of elongation | <土10 | <土10 | <土10 | <土10 | |
| Permanent deformation at constant extension 300% x 90°C x 168H | <5% | <5% | <5% | <5% | |
| Dielectric constant at 100HZ | 3.03 | 3.03 | 3.03 | 2 95 | |
| Dissipation factor at100HZ | 0.0029 | 0.0029 | 0.0029 | 0.0029 | |
| Resistance to electric leakage and marking | 1A3.5 | 1A3.5 | 1A3.5 | 1A4.5 | |
| DielectricStrength (kV/mm) | 24 | 24 | 22 | 23 | |
| VolumeResistivity (Ω·cm) | 1.0 *1015 | 1.0 *1015 | 1.0 *1015 | 1.0 *1015 | |