GA-2041WY
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: A/B ratio is adjustable, 130°C x 5min x 15MPa
| Product parameters | |||||
| Product | GA-2041WY | GA-2051WY | GA-2061WY | GA-2071WY | |
| Appearance | Light grey | Light grey | Dark grey | Light grey | |
| A/Bratio | 2:100 | 2:100 | 1:1 | 2:100 | |
| Viscosity(Pa.s) | 14-20 | 140-160 | 70-90 | 140-160 | |
| Hardness (ShoreA) | 45 | 50 | 65 | 70 | |
| Density(g/cm3) | 1.3 | 1.36 | 1.6 | 1.5 | |
| Tensile strength (MPa) | 2.5 | 3.0 | 3.0 | 3.0 | |
| Elongation(%) | 200 | 300 | 170 | 140 | |
| Tear strength (kN/m) | 7 | 7 | 7 | 8 | |
| Flame class | UL94V-0 | UL94V-0 | UL94V-0 | UL94V-0 | |