Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa.
| Product parameters | ||||||
| Product | GA-2230 | GA-2240 | GA-2250 | GA-2260 | GA-2270 | |
| Appearance | Transparent | |||||
| Viscosity(Pa.s) | 10 | 10 | 8 | 5 | 5 | |
| Hardness (ShoreA) | 30 | 40 | 50 | 60 | 70 | |
| Density(g/cm3) | 1.01 | 1.01 | 1.01 | 1.01 | 1.01 | |
| Tensile strength (MPa) | 4.0 | 4.5 | 6.0 | 7.0 | 8.0 | |
| Elongation(%) | 150 | 170 | 220 | 150 | 80 | |
| Tear strength (kN/m) | 12 | 14 | 20 | 18 | 10 | |
| Linear shrinkage(%) | 2.1 | 2.1 | 2.1 | 2.0 | 2.0 | |
| Transmittance(%) | 94 | 94 | 94 | 94 | 94 | |