Test: A/B ratio of 1 :1, 130°C x 5min x 15MPa
| Product parameters | |||||
| Product | GA-2135-15 | GA-2135-25 | GA-2135-35 | GA-2135-45 | |
| Appearance | Translucent | ||||
| Viscosity(Pa.s) | 60 | 30 | 38 | 30 | |
| Hardness (ShoreA) | 18 | 26 | 35 | 48 | |
| Density(g/cm3) | 1.03 | 1.06 | 1.06 | 1.10 | |
| Tensile strength (MPa) | 2.5 | 2.8 | 4.2 | 5.5 | |
| Elongation(%) | 400 | 380 | 330 | 250 | |
| Tear strength (kN/m) | 8 | 9.5 | 11.5 | 16 | |
| Linearshrinkage(%) | 1.7 | 1.7 | 1.7 | 1.7 | |