GA-2029X
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 130°C x 5min x 15MPa
| Product parameters | |||||||
| Product | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | GA-2029X | |
| Appearance | Translucent | ||||||
| Viscosity(Pa.s) |
A:1000 B:2000 |
A:2000 B:3000 |
A:2000 B:4000 |
A:2000 B:4000 |
A:2000 B:4000 |
A:5000 B:6000 |
|
| Hardness (ShoreA) | 20 | 30 | 40 | 50 |
60 |
70 |
|
| Density(g/cm3) | 5 | 7 | 8 | 8 | 8 |
7 |
|
| Tensile strength (MPa) | 900 |
600 |
550 |
500 |
400 |
250 |
|
| Elongation(%) | 10 | 10 | 15 | 25 | 25 |
30 |
|
| Tear strength (kN/m) | 16 | 30 | 35 |
40 | 35 |
30 |
|