GA-8142P
Herchy
| Availability: | |
|---|---|
| Quantity: | |
Test: 1.0% of curing agent (45% paste of DBPMH in silicone gum), 175°C x 5min x 15MPa
| Product parameters | ||||
| Product | GA-8142P |
GA-8152P | GA-8162P | GA-8172P |
| Appearance | White |
|||
| Williamplasticity |
160 |
200 |
250 |
270 |
| Hardness (ShoreA) |
40 |
50 |
60 |
70 |
| Density(g/cm3) | 1.3 |
1.28 |
1.28 |
1.42 |
| Tensile strength (MPa) |
6.5 |
9 |
9 |
7.5 |
| Elongation(%) | 550 |
650 |
700 |
300 |
| Tear strength (kN/m) | 18 |
24 |
45 |
23 |