GA-81×2P roba silikoni idaduro ina pẹlu agbara giga (HCR)

Ohun elo: ina retardant oriṣiriṣi fun awọn ẹya adaṣe, igbanu alapapo ti kondisona, ati gasiketi ina, bbl
Awọn ẹya ara ẹrọ: agbara giga, halogen-ọfẹ ati imuduro ina ti ko ni imi-ọjọ, kọja ijẹrisi ti RoHS ati REACH.
  • GA-8142P

  • Herchy

Wiwa:
Opoiye:

Idanwo: 1.0% ti oluranlowo imularada (45% lẹẹ DBPMH ni silikoni gomu), 175°C x 5min x 15MPa


Ọja sile
Ọja GA-8142P
GA-8152P GA-8162P GA-8172P
Ifarahan Funfun
Williamplasticity
160
200
250
270
Lile ( ShoreA)
40
50
60
70
Ìwúwo (g/cm3) 1.3
1.28
1.28
1.42
Agbara fifẹ (MPa)

6.5
9
9
7.5
Ilọsiwaju(%) 550
650
700
300
Agbara omije (kN/m) 18
24
45
23









Ti tẹlẹ: 
Itele: 

Awọn ọna asopọ kiakia

Awọn ọja WA

IBI IWIFUNNI

Fi kun: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tẹli / WhatsApp / Skype: +86 15221953351
Aṣẹ-lori-ara     2023 Shanghai Herchy Rubber Co., Ltd. Maapu aaye |   Asiri Afihan | Atilẹyin Nipasẹ Leadong.