GA-8142P
Herchy nga bwe kiri
| Ebiriwo: | |
|---|---|
| Omuwendo: | |
Okugezesa: 1.0% eky’ekirungo ekiwonya (45% ekikuta kya DBPMH mu silicone gum), 175°C x 5min x 15MPa
| Ebipimo by’ebintu ebikolebwa | ||||
| Ekyamaguzi | GA-8142P |
GA-8152P | GA-8162P | GA-8172P |
| Endabika | Kyeeru |
|||
| Obuveera bwa William |
160 |
200 |
250 |
270 |
| Obukaluba (ShoreA) . |
40 |
50 |
60 |
70 |
| Obugumu(g/cm3) . | 1.3 |
1.28 |
1.28 |
1.42 |
| Amaanyi g’okusika (MPa) . |
6.5 |
9 |
9 |
7.5 |
| Okuwanvuwa(%) . | 550 |
650 |
700 |
300 |
| Amaanyi g’okukutuka (kN/m) . | 18 |
24 |
45 |
23 |