GA-81×2P Silicone rɔba a ogya ntumi nhyew a ahoɔden kɛse (HCR) wom .

Dwumadi: ogya retardant ahorow ahorow ma auto afã horow, ɔhyew bɛlt a mframa conditioner,ne ogya retardant gasket, ne nea ɛkeka ho.
Keyfeatures:ahoɔden a ɛkorɔn,halogen-free ne sulfur-free ogya retardant, twa nokwaredi a RoHS ne REACH.
  • GA-8142P na ɛwɔ hɔ

  • Herchy a ɔyɛ ɔbarima

Nea Ɛwɔ Hɔ:
Dodow:

Sɔhwɛ: 1.0% a wɔde sa yareɛ (45% a wɔde DBPMH a wɔde ahyɛ silicone gum mu), 175°C x 5min x 15MPa


Nneɛma a wɔyɛ no parameters
Adwadeɛ GA-8142P na ɛwɔ hɔ
GA-8152P na ɛwɔ hɔ GA-8162P na ɛwɔ hɔ GA-8172P na ɛwɔ hɔ
Mmaeɛ Fitaa
Williamplasticity a wɔde yɛ nneɛma
160
200
250
270
Nneɛma a ɛyɛ den (ShoreA) .
40
50
60
70
Nsuo a ɛyɛ den(g/cm3) . 1.3
1.28
1.28
1.42
Ahoɔden a wɔde twe ade (MPa) .

6.5
9
9
7.5
Ntrɛwmu(%) . 550
650
700
300
Ahoɔden a ɛtetew mu (kN/m) . 18
24
45
23









Dada: 
Deɛ ɛdi hɔ: 

NKYERƐKYERƐMU A ƐYƐ NTƐM

NKYERƐKYERƐMU A ƐFA NKYERƐKYERƐMU HO

Fa ka ho: No.33, Ɔkwan 159, Taiye Kwan, Fengxian Mantam, Shanghai
Tɛlɛ / WhatsApp / Skype: +86 15221953351 wobɛtumi akyerɛw wo din
Nneɛma a wɔde yɛ adwuma     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap a Wɔde Di Dwuma |   Kokoam Nsɛm Ho Nhyehyɛe | Mmoa a Wɔde Ma Leadong na ɛwɔ hɔ.