GA-8142P irratti kan argamu
Herchy jedhamuun beekama
| Argamuu: | |
|---|---|
| Baay’ina: . | |
Qormaata: 1.0% qoricha fayyisuu (45% paastaa DBPMH silikoonii gogaa keessatti), 175°C x 5min x 15MPa
| Parameetaroota oomishaa | ||||
| Oomisha | GA-8142P irratti kan argamu |
GA-8152P irratti kan argamu | GA-8162P irratti kan argamu | GA-8172P irratti kan argamu |
| Mul'ina | Adii |
|||
| Wiliyaampilaastikii |
160 |
200 |
250 |
270 |
| Jabina (ShoreA) . |
40 |
50 |
60 |
70 |
| Dandeettii(g/cm3) . | 1.3 |
1.28 |
1.28 |
1.42 |
| Jabina harkisaa (MPa) . |
6.5 |
9 |
9 |
7.5 |
| Dheersuu(%) . | 550 |
650 |
700 |
300 |
| Jabina ciccituu (kN/m) . | 18 |
24 |
45 |
23 |