GA-8142P
Herchy
| Beskikberens: | |
|---|---|
| Kwantiteit: | |
Test: 1,0% ferhurdingsmiddel (45% pasta fan DBPMH yn silikongom), 175 °C x 5min x 15MPa
| Produkt parameters | ||||
| Produkt | GA-8142P |
GA-8152P | GA-8162P | GA-8172P |
| Ferskining | Wyt |
|||
| Williamplasticity |
160 |
200 |
250 |
270 |
| Hardheid (ShoreA) |
40 |
50 |
60 |
70 |
| Tichtheid (g/cm3) | 1.3 |
1.28 |
1.28 |
1.42 |
| Treksterkte (MPa) |
6.5 |
9 |
9 |
7.5 |
| Ferlinging (%) | 550 |
650 |
700 |
300 |
| Tear sterkte (kN/m) | 18 |
24 |
45 |
23 |