ʻO GA-81×2P ʻO ka lāʻau silikika pale ahi me ka ikaika kiʻekiʻe (HCR)

Hoʻohana: flame retardant miscellaneous no nā ʻāpana kaʻa, kāʻei wela o ka ea, a me ka gasket retardant ahi, etc.
ʻO nā hiʻohiʻona nui: ikaika kiʻekiʻe, halogen-free a me ka sulfur-free flame retardant, hele i ka hōʻoia o RoHS a me REACH.
  • GA-8142P

  • Herchy

Loaʻa:
Nui:

Ho'āʻo: 1.0% o ka lāʻau lapaʻau (45% paʻi o DBPMH i loko o ka silicone gum), 175°C x 5min x 15MPa


Nā palena huahana
Huahana GA-8142P
GA-8152P GA-8162P GA-8172P
Ka nana aku Keʻokeʻo
Williamplasticity
160
200
250
270
Paʻakikī (ShoreA)
40
50
60
70
Māmā (g/cm3) 1.3
1.28
1.28
1.42
Ka ikaika uʻi (MPa)

6.5
9
9
7.5
Elongation(%) 550
650
700
300
Kaha waimaka (kN/m) 18
24
45
23









Mua: 
Aʻe: 

NUI WIWIKI

KO MAKOU HANA

IKE HOPE

Hoʻohui: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Kuleana kope     2023 Shanghai Herchy Rubber Co., Ltd. Palapala kahua |   Kulekele pilikino | Kākoʻo Na Leadong.