GA-81×2P Flame-retardant silicone roba tare da babban ƙarfi (HCR)

Application: harshen wuta retardant iri-iri ga auto sassa, dumama bel na kwandishan, da harshen wuta retardant gasket, da dai sauransu.
Maɓalli: babban ƙarfi, halogen-free kuma sulfur-free harshen retardant, wuce da Tantancewar RoHS da REACH.
  • GA-8142P

  • Herchy

samuwa:
Yawan:

Gwaji: 1.0% na wakili mai warkarwa (45% manna DBPMH a cikin danko silicone), 175°C x 5min x 15MPa


Siffofin samfur
Samfura GA-8142P
GA-8152P GA-8162P GA-8172P
Bayyanar Fari
Williamplasticity
160
200
250
270
Hardness (ShoreA)
40
50
60
70
Girma (g/cm3) 1.3
1.28
1.28
1.42
Ƙarfin ɗaure (MPa)

6.5
9
9
7.5
Tsawaita(%) 550
650
700
300
Ƙarfin hawaye (kN/m) 18
24
45
23









Na baya: 
Na gaba: 

SAUKAR HANYA

KAYANMU

BAYANIN HULDA

Ƙara: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Haƙƙin mallaka     2023 Shanghai Herchy Rubber Co., Ltd. Taswirar yanar gizo |   Manufar Keɓantawa | Taimako Ta Leadong.