GA-81×2P Flame-retardant silicone roba nwere ike dị elu (HCR)

Ngwa: ire ọkụ retardant dị iche iche maka akpaaka akụkụ, kpo oku belt nke ikuku conditioner, na ọkụ retardant gasket, wdg.
Isi ihe: ike dị elu, enweghị halogen na ire ọkụ na-enweghị sọlfọ, gafere nyocha nke RoHS na REACH.
  • GA-8142P

  • Herchy

Nnweta:
Ọnụọgụ:

Nnwale: 1.0% nke onye na-agwọ ọrịa (45% tapawa nke DBPMH na silicone gum), 175°C x 5min x 15MPa


Ngwa ngwaahịa
Ngwaahịa GA-8142P
GA-8152P GA-8162P GA-8172P
Ọdịdị Ọcha
Williamplasticity
160
200
250
270
Isi ike (ShoreA)
40
50
60
70
Njupụta (g/cm3) 1.3
1.28
1.28
1.42
Ike tensile (MPa)

6.5
9
9
7.5
Mgbatị(%) 550
650
700
300
Ike akwa mmiri (kN/m) 18
24
45
23









Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.