U teng: Lehae GA - Lihlahisoa 81 Synthesis Rubber 2P VMQ Silicone × rabara ea silicone e sa chesehang mollo e nang le matla a phahameng (HCR)

loading

Arolelana le:
konopo ea ho arolelana facebook
konopo ea ho arolelana twitter
konopo ea ho arolelana line
konopo ea ho arolelana wechat
konopo ea ho arolelana linkedin
konopo ea ho arolelana pinterest
konopo ea ho arolelana whatsapp
Share this share konopo

GA-81 × 2P rabara ea silicone e thibelang mollo e nang le matla a phahameng (HCR)

Ts'ebeliso: mefuta e fapaneng ea retardant bakeng sa likarolo tsa koloi, lebanta le futhumatsang la moea o futhumatsang moea, le gasket e thibelang malakabe, jj.
Litšobotsi tsa bohlokoa: matla a phahameng, halogen e se nang halogen ebile e se na sebabole retardant, fetisa netefatso ea RoHS le REACH.
  • GA-8142P

  • Herchy

Boteng:
Bongata:

Teko: 1.0% ea moemeli oa ho folisa (45% peista ea DBPMH ka har'a chese ea silicone), 175 ° C x 5min x 15MPa


Lihlahisoa tsa lihlahisoa
Sehlahisoa GA-8142P
GA-8152P GA-8162P GA-8172P
Ponahalo Bosoeu
Williamplasticity
160
200
250
270
Ho thatafala (LebopoA)
40
50
60
70
Boima ba 'mele(g/cm3) 1.3
1.28
1.28
1.42
Tensile Matla (MPa)

6.5
9
9
7.5
Elongation(%) 550
650
700
300
Matla a ho lla (kN/m) 18
24
45
23









E fetileng: 
E 'ngoe: 

LIEKETSENG POTLAKO

LIHLAHISO TSA RONA

MOKHOA OA PUISANO

Eketsa: No.33, Lane 159, Taiye Road, Setereke sa Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sebaka sa marang-rang |   Leano la Lekunutu | Tšehetso Ka Leadong.