GA-8142P. Ƒe 1999 me
Herchy ƒe ame
| Nusiwo Li: | |
|---|---|
| Agbɔsɔsɔ: | |
Dodokpɔ: 1.0% ƒe atike si daa gbe le ame ŋu (45% ƒe atike si wotsɔ DBPMH wɔe le silicon-gum me), 175°C x 5min x 15MPa
| Nusiwo wowɔ ƒe nɔnɔmewo | ||||
| Nu si wowɔ | GA-8142P. Ƒe 1999 me |
GA-8152P ƒe agbalẽa | GA-8162P | GA-8172P |
| Dzedzeme | Ɣi |
|||
| Williamplasticity ƒe dɔwɔwɔ |
160 |
200 |
250 |
270 |
| Sesẽme (ƑutaA) . |
40 |
50 |
60 |
70 |
| Eƒe kpekpeme(g/cm3) . | 1.3 |
1.28 |
1.28 |
1.42 |
| Ŋusẽ si wotsɔna ƒoa nu (MPa) . |
6.5 |
9 |
9 |
7.5 |
| Elongation(%) ƒe didime . | 550 |
650 |
700 |
300 |
| Aɖatsi ƒe ŋusẽ (kN/m) . | 18 |
24 |
45 |
23 |