GA-8142P
Herchy
| Avanoa: | |
|---|---|
| Aofaiga: | |
Su'ega: 1.0% o le vaila'au fa'amalolo (45% fa'apipi'i o le DBPMH i le pulu silicone), 175°C x 5min x 15MPa
| Fa'atauga o oloa | ||||
| Oloa | GA-8142P |
GA-8152P | GA-8162P | GA-8172P |
| Fa'aaliga | Lanu pa'epa'e |
|||
| Williamplasticity |
160 |
200 |
250 |
270 |
| Malosi (ShoreA) |
40 |
50 |
60 |
70 |
| Malosi (g/cm3) | 1.3 |
1.28 |
1.28 |
1.42 |
| Malosi fa'amalosi (MPa) |
6.5 |
9 |
9 |
7.5 |
| Fa'atele(%) | 550 |
650 |
700 |
300 |
| Malosi o loimata (kN/m) | 18 |
24 |
45 |
23 |