Tel: +8615221953351   E-mail: info@herchyrubber.com
PRODUCTS
You are here: Home » Products » Synthesis Rubber » VMQ Silicone » GA-81×2P Flame-retardant silicone rubber with high strength (HCR)

loading

Share to:
facebook sharing button
twitter sharing button
line sharing button
wechat sharing button
linkedin sharing button
pinterest sharing button
whatsapp sharing button
sharethis sharing button

GA-81×2P Flame-retardant silicone rubber with high strength (HCR)

Application: flame retardant miscellaneous for auto parts, heating belt of air conditioner,and flame retardant gasket, etc.
Keyfeatures:high strength,halogen-free and sulfur-free flame retardant, pass the authentication of RoHS and REACH.
  • GA-8142P

  • Herchy

Availability:
Quantity:

Test: 1.0% of curing agent (45% paste of DBPMH in silicone gum), 175°C x 5min x 15MPa


Product parameters
ProductGA-8142P
GA-8152PGA-8162PGA-8172P
AppearanceWhite
Williamplasticity
160
200
250
270
Hardness (ShoreA)
40
50
60
70
Density(g/cm3)1.3
1.28
1.28
1.42
Tensile strength (MPa)

6.5
9
9
7.5
Elongation(%)550
650
700
300
Tear strength (kN/m)18
24
45
23









Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.